Plastic Granules
Apec 1795 PC Resin Heat Resistant Grade
Covestro Apec 1795 is a premium heat-resistant copolycarbonate resin. Its low viscosity and easy-release properties enable fast, efficient injection molding of complex, high-precision parts that withstand continuous temperatures up to 173°C (VST). Perfect for automotive lighting and technical components.
Download PDF
ISO TDS
Typical property data
Physical Properties (Rheological)
- Melt Volume-Flow Rate (330 °C/2.16 kg): 30 cm³/10 min (ISO 1133)
- Melt Mass-Flow Rate (330 °C/2.16 kg): 31 g/10 min (ISO 1133)
- Molding Shrinkage (Parallel): 0.8% (ISO 294-4)
- Molding Shrinkage (Normal): 0.8% (ISO 294-4)
Mechanical properties (23 °C/50 % r. h.)
- Tensile Modulus (1 mm/min): 2350 MPa (ISO 527-1, -2)
- Yield Stress (50 mm/min): 71 MPa (ISO 527-1, -2)
- Yield Strain (50 mm/min): 6.6% (ISO 527-1, -2)
- Nominal Strain at Break (50 mm/min): > 50% (ISO 527-1, -2)
- Flexural Modulus (2 mm/min): 2400 MPa (ISO 178)
- Flexural Strength (2 mm/min): 105 MPa (ISO 178)
- Ball Indentation Hardness: 125 N/mm² (ISO 2039-1)
Thermal Properties
- Temperature of Deflection Under Load (1.80 MPa): 148 °C (ISO 75-1, -2)
- Temperature of Deflection Under Load (0.45 MPa): 162 °C (ISO 75-1, -2)
- Vicat Softening Temperature (50 N, 120 °C/h): 173 °C (ISO 306)
- Relative Temperature Index (Tensile Strength): 140 °C (UL 746B)
- Coefficient of Linear Thermal Expansion (Parallel, 23–55 °C): 0.65 × 10⁻⁴/K (ISO 11359-1, -2)
- Burning Behavior UL 94 (1.5 mm): HB Class (UL 94)
- Glow Wire Test (GWFI): 850 °C (IEC 60695-2-12)
Electrical properties (23 °C/50 % r. h.)
- Relative Permittivity (100 Hz): 3 (IEC 60250)
- Dissipation Factor (100 Hz): 10 × 10⁻⁴ (IEC 60250)
- Volume Resistivity: 1 × 10¹⁵ Ω·m (IEC 62631-3-1)
- Surface Resistivity: 1 × 10¹⁶ Ω (IEC 62631-3-2)
- Electrical Strength (1 mm): 35 kV/mm (IEC 60243-1)
- Comparative Tracking Index (CTI, Solution A): 250 Rating (IEC 60112)
Other Properties (23 °C)
- Water Absorption (Saturation Value): 0.3% (ISO 62)
- Water Absorption (Equilibrium Value, 50% r.h.): 0.12% (ISO 62)
- Density: 1170 kg/m³ (ISO 1183-1)
Material-Specific Properties
- Refractive Index (Procedure A): 1.576 (ISO 489)
- Luminous Transmittance (Clear Transparent Materials, 1 mm): 89% (ISO 13468-2)
Use & Applications
- Injection molding
- Covers for brake lights and indicator lights
- Headlamp reflectors
- Headlamp bezels
Features & Benefits
Effortless High-Precision Molding
Apec® 1795’s exceptionally low melt viscosity (30 cm³/10min) ensures easy filling of intricate, thin-walled molds. This reduces cycle times, minimizes injection pressure, and lowers energy consumption, boosting your production efficiency and part yield.
Superior Heat Resistance & Stability
Withstanding high continuous service temperatures (Vicat 173°C, HDT 146°C @ 1.8 MPa), Covestro APEC Polycarbonate 1795 maintains dimensional stability and performance in hot environments like under-hood automotive applications, preventing warping or failure.
Reliable Dimensional Consistency
Featuring low and balanced shrinkage (0.8% both parallel/normal), Apec 1795 ensures predictable, precise final part dimensions critical for tight-tolerance assemblies like bezels and reflectors, reducing post-molding adjustments and scrap.