Typical property data
Physical Properties (Rheological)
- Melt Volume-Flow Rate (MVR): 18 cm³/10 min (330 °C/2.16 kg, ISO 1133)
- Melt Mass-Flow Rate (MFR): 19 g/10 min (330 °C/2.16 kg, ISO 1133)
- Molding Shrinkage (Parallel/Normal): 0.85% (60x60x2 mm³, ISO 294-4)
Mechanical Properties (23 °C/50% r.h.)
- Tensile Modulus: 2350 MPa (1 mm/min, ISO 527-1,-2)
- Yield Stress: 72 MPa (50 mm/min, ISO 527-1,-2)
- Yield Strain: 6.7% (50 mm/min, ISO 527-1,-2)
- Nominal Strain at Break: >50% (50 mm/min, ISO 527-1,-2)
- Flexural Modulus: 2400 MPa (2 mm/min, ISO 178)
- Flexural Strength: 108 MPa (2 mm/min, ISO 178)
- Ball Indentation Hardness: 127 N/mm² (ISO 2039-1)
Thermal Properties
- Temperature of Deflection Under Load (1.8 MPa): 157 °C (ISO 75-1,-2)
- Temperature of Deflection Under Load (0.45 MPa): 174 °C (ISO 75-1,-2)
- Vicat Softening Temperature: 183 °C (50 N; 120 °C/h, ISO 306)
- Relative Temperature Index (Tensile Strength): 150 °C (UL 746B)
- Coefficient of Linear Thermal Expansion (Parallel/Normal, 23-55 °C): 0.65 × 10⁻⁴/K (ISO 11359-1,-2)
Electrical Properties (23 °C/50% r.h.)
- Relative Permittivity: 2.9 (100 Hz, IEC 60250); 2.8 (1 MHz, IEC 60250)
- Dissipation Factor: 10 × 10⁻⁴ (100 Hz, IEC 60250); 80 × 10⁻⁴ (1 MHz, IEC 60250)
- Volume Resistivity: 1 × 10¹⁵ Ohm·m (IEC 62631-3-1)
- Surface Resistivity: 1 × 10¹⁶ Ohm (IEC 62631-3-2)
- Electrical Strength: 35 kV/mm (1 mm, IEC 60243-1)
- Comparative Tracking Index (CTI): 300 (Solution A, IEC 60112)
Other Properties (23 °C)
- Water Absorption (Saturation): 0.3% (Water at 23 °C, ISO 62)
- Water Absorption (Equilibrium): 0.12% (23 °C, 50% r.h., ISO 62)
- Density: 1150 kg/m³ (ISO 1183-1)
Material Specific Properties
- Refractive Index: 1.573 (Procedure A, ISO 489)
- Luminous Transmittance: 89% (1 mm, ISO 13468-2)
Processing Conditions
- Injection Molding Melt Temperature: 330-340 °C (ISO 294)
- Mold Temperature: 120-140 °C (ISO 294)
- Drying Conditions: 130 °C for 2-3 hours (Moisture Content ≤ 0.02%)
Features & Benefits
High Flow, Fast Cycling
Apec® 1895’s superior melt flow (18 cm³/10 min) fills intricate molds quickly, reducing cycle times by up to 15% and boosting production efficiency. Perfect for thin-walled automotive lenses.
Heat & Warpage Resistance
It withstands 183°C softening temps and offers low thermal expansion (0.65×10⁻⁴/K), ensuring dimensional stability under heat. Ideal for LED reflectors near high-temperature sources.
Effortless Mold Release
Easy-release properties minimize sticking and surface defects, cutting demolding time and scrap rates. Eliminates finishing costs for glossy light covers.
Use & Applications
- Injection molding
- Covers for brake lights and indicator lights
- Recessed light fixtures/reflectors
- Raised brake lights
- Headlamp reflectors
- Headlamp bezels