Covestro Apec® 2095 PC Resin

covestro apec

Apec 2095 PC Resin Heat Resistant Grade

Covestro Apec 2095 is a high-heat copolycarbonate resin. With high viscosity, easy-flow processing, and exceptional heat resistance (Vicat softening: 203°C), it excels in automotive and lighting components where durability and precision matter. Ideal for injection molding complex parts.

Download PDF

Typical property data

Physical Properties (Rheological)
  • Melt Volume-Flow Rate (MVR): 8 cm³/10 min (330 °C/2.16 kg, ISO 1133)
  • Mold Shrinkage: 1.05% (parallel/normal, ISO 294-4)
Mechanical Properties (23 °C/50% r. h.)
  • Tensile Modulus: 2400 MPa (1 mm/min, ISO 527-1,-2)
  • Yield Stress: 75 MPa (50 mm/min, ISO 527-1,-2)
  • Yield Strain: 6.8% (50 mm/min, ISO 527-1,-2)
  • Flexural Modulus: 2450 MPa (2 mm/min, ISO 178)
  • Flexural Strength: 110 MPa (2 mm/min, ISO 178)
  • Ball Indentation Hardness: 130 N/mm² (ISO 2039-1)
Thermal Properties
  • Deflection Temperature under Load (1.80 MPa): 173 °C (ISO 75-1,-2)
  • Vicat Softening Temperature: 203 °C (50 N; 120 °C/h, ISO 306)
  • Burning Behavior: UL 94 HB (1.5 mm, UL 94)
  • Glow Wire Flammability Index (GWFI): 800 °C (2.0 mm, IEC 60695-2-12)
Electrical Properties (23 °C/50% r. h.)
  • Relative Permittivity: 2.9 (100 Hz, IEC 60250); 2.8 (1 MHz, IEC 60250)
  • Electrical Strength: 35 kV/mm (1 mm, IEC 60243-1)
  • Comparative Tracking Index (CTI): 600 (Solution A, IEC 60112)
Other Properties (23 °C)
  • Water Absorption (Saturation): 0.3% (ISO 62)
  • Density: 1130 kg/m³ (ISO 1183-1)
Material Specific Properties
  • Refractive Index: 1.566 (Procedure A, ISO 489)
  • Luminous Transmittance (Clear Transparent Materials): 90% (1 mm, ISO 13468-2)
Process Guide
  • Injection Molding Melt Temperature: 330–340 °C (Standard: 335 °C, ISO 294)
  • Mold Temperature: 130–150 °C
  • Drying Temperature: 130 °C for 2–3 hours (Max. Moisture Content: ≤ 0.02%)
  • Injection Velocity: 200 mm/s (ISO 294)
  • Barrel Temperature Range: 295–335 °C

Use & Applications

  • Injection molding
  • Covers for brake lights and indicator lights
  • Recessed light fixtures/reflectors
  • Raised brake lights
  • Headlamp reflectors
  • Headlamp bezels
covestro apec

Features & Benefits

Exceptional Heat Resistance

Apec® 1695 withstands temperatures up to 158°C (VST/B 120), ensuring stability in high-heat environments like headlamp assemblies. Prevents warping during prolonged use.

Easy Flow & Release

Optimized melt flow (45 cm³/10 min) reduces injection pressure and cycle times. Simplifies molding of thin-walled parts like light covers without sticking.

Superior Dimensional Stability

Low, uniform shrinkage (0.75% parallel/normal) maintains tight tolerances in complex geometries. Critical for seamless fit in automotive reflectors.

covestro apec