Covestro Apec® 2097 PC Resin

covestro apec

Apec 2097 PC Resin Heat Resistant Grade

Covestro Apec® 2097 is a high-heat, UV-stabilized copolycarbonate resin engineered for demanding applications. With exceptional flow (MVR 8 cm³/10 min), easy-release properties, and a Vicat softening temperature of 202°C, it delivers reliability for precision injection-molded components like automotive lighting.

Associated Documents

ISO TDS

Typical property data

Physical Properties (Rheological)
  • Melt Volume-Flow Rate (330 °C/2.16 kg): 8 cm³/10 min (ISO 1133)
  • Mold Shrinkage (Parallel/Normal, 60x60x2 mm³): 0.9% (ISO 294-4)
Mechanical Properties (23 °C/50% r. h.)
  • Tensile Modulus: 2400 MPa (ISO 527-1, -2)
  • Yield Stress: 75 MPa (ISO 527-1, -2)
  • Yield Strain: 6.9% (ISO 527-1, -2)
  • Nominal Strain at Break: >50% (ISO 527-1, -2)
  • Flexural Modulus: 2450 MPa (ISO 178)
  • Flexural Strength: 110 MPa (ISO 178)
  • Ball Indentation Hardness: 130 N/mm² (ISO 2039-1)
Thermal Properties
  • Deflection Temperature under Load (1.80 MPa): 172 °C (ISO 75-1, -2)
  • Deflection Temperature under Load (0.45 MPa): 191 °C (ISO 75-1, -2)
  • Vicat Softening Temperature (50 N; 120 °C/h): 202 °C (ISO 306)
  • Coefficient of Linear Thermal Expansion (Parallel/Normal, 23–55 °C): 6.5 × 10⁻⁵ K⁻¹ (ISO 11359-1, -2)
  • Burning Behavior: HB (1.5 mm) (UL 94)
  • Glow Wire Test (GWFI): 800 °C (IEC 60695-2-12)
Electrical Properties (23 °C/50% r. h.)
  • Relative Permittivity (100 Hz): 2.9 (IEC 60250)
  • Relative Permittivity (1 MHz): 2.8 (IEC 60250)
  • Dissipation Factor (100 Hz): 10 × 10⁻⁴ (IEC 60250)
  • Dissipation Factor (1 MHz): 90 × 10⁻⁴ (IEC 60250)
  • Volume Resistivity: 1 × 10¹⁵ Ohm·m (IEC 62631-3-1)
  • Surface Resistivity: 1 × 10¹⁶ Ohm (IEC 62631-3-2)
  • Electrical Strength: 35 kV/mm (IEC 60243-1)
  • Comparative Tracking Index (Solution A): 600 (IEC 60112)
Other Properties (23 °C)
  • Density: 1130 kg/m³ (ISO 1183-1)
  • Water Absorption (Equilibrium Value, 23 °C, 50 % RH): 0.12% (ISO 62)
  • Water Absorption (Saturation Value, Water at 23 °C): 0.3% (ISO 62)
Material Specific Properties
  • Refractive Index: 1.566 (ISO 489)
  • Luminous Transmittance (1 mm, Clear Transparent): 89% (ISO 13468-2)
Process Guide
  • Injection Molding Melt Temperature: 330–340 °C (ISO 294)
  • Mold Temperature: 130–150 °C
  • Drying Temperature: 130 °C
  • Drying Time: 2–3 hours
  • Moisture Content (Max): ≤ 0.02%
  • Injection Velocity: 200 mm/s
  • Hold Pressure (% of Injection Pressure): 50–75%

Features & Benefits

High Heat Resistance & Stability

Apec® 2097 withstands temperatures up to 202°C (VST), preventing deformation in high-stress environments. Ideal for automotive parts exposed to engine heat or intense lighting systems.

UV Protection for Longevity

UV-stabilized to resist yellowing and degradation, Covestro Apec 2097 maintains optical clarity (89% transmittance) for outdoor applications like headlamp lenses exposed to sunlight.

Easy-Release Molding Efficiency

Low-stick formulation reduces demolding time and minimizes part damage, streamlining production of complex geometries like lamp covers while cutting manufacturing costs.

covestro apec

Use & Applications

  • Injection molding
  • Lamp covers
  • Headlamp lenses
covestro apec

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.