Covestro Bayblend® 2953 PC/ABS

covestro bayblend pc abs blend

Bayblend 2953 Electroplating Grade PC/ABS

Bayblend 2953 is an advanced (PC+ABS) blend engineered for electroplating applications, featuring a Vicat softening temperature of 113°C. This high-performance resin combines robustness, thermal stability, and exceptional surface quality, making it ideal for industrial components requiring durability and aesthetic appeal.

Download PDF

Typical property data

Physical Properties (Rheological)
  • Melt Volume-Flow Rate (MVR): 14 cm³/10 min (260 °C, 5 kg) (ISO 1133)
Mechanical properties (23 °C/50 % r. h.)
  • Tensile Modulus: 2,100 MPa (ISO 527-1, -2)
  • Yield Stress: 44 MPa (ISO 527-1, -2)
  • Yield Strain: 3.6% (ISO 527-1, -2)
  • Nominal Strain at Break: >50% (ISO 527-1, -2)
  • Stress at Break: 47 MPa (ISO 527-1, -2)
  • Flexural Modulus: 2,200 MPa (ISO 178)
  • Flexural Stress at 3.5% Strain: 65 MPa (ISO 178)
  • Izod Notched Impact Strength:
    • 23 °C: 46 kJ/m² (ISO 180/A)
    • -30 °C: 35 kJ/m² (ISO 180/A)
Thermal properties
  • Temperature of Deflection Under Load (Tg):
    • 1.80 MPa: 90 °C (ISO 75-1, -2)
    • 0.45 MPa: 110 °C (ISO 75-1, -2)
  • Vicat Softening Temperature:
    • 50 °C/h: 108 °C (ISO 306)
    • 120 °C/h: 113 °C (ISO 306)
Other properties (23 °C)
  • Density: 1,110 kg/m³ (ISO 1183-1)
Process Guide
  • Melt Temperature Range: 260–280 °C (Standard: 270 °C)
  • Barrel Temperatures:
    • Rear: 230–240 °C
    • Middle: 235–245 °C
    • Front: 240–270 °C
    • Nozzle: 265–275 °C
  • Mold Temperature: 70–90 °C
  • Hold Pressure (% Injection Pressure): 50–75%
  • Plastic Back Pressure: 50–150 bar
  • Peripheral Screw Speed: 0.05–0.2 m/s
  • Drying Conditions:
    • Air Drying Temperature: 80 °C
    • Drying Time: 4 hours
    • Max Moisture Content: ≤0.02%

Use & Applications

  • Injection molding
  • Electroplating
covestro bayblend pc abs blend

Features & Benefits

Superior Electroplating Performance

Bayblend® 2953 offers flawless adhesion for metallic finishes, ensuring brilliant chrome-like surfaces without peeling—perfect for automotive trims or luxury electronics.

High Impact Resistance

With 46 kJ/m² notched impact strength at 23°C (and 35 kJ/m² at -30°C), it withstands drops and shocks, reducing part failure in tools or consumer devices.

Optimized Processing Efficiency

Precise melt temperatures (260–280°C) and quick drying (4 hours at 80°C) cut cycle times and energy costs in injection molding.

covestro bayblend pc abs blend

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.