Plastic Granules
Bayblend® FR1514 PC/ABS Flame Retardant Grade
Bayblend FR1514 is a flame-retardant PC+ABS blend engineered for high-heat applications. With UL 94 V-0 certification at 1.5 mm, Vicat softening at 136°C, and exceptional impact resistance, it’s ideal for energized electrical components demanding safety and durability.
Typical property data
Physical Properties (Rheological)
- Melt volume-flow rate: 19 cm³/10 min (260 °C/5 kg, ISO 1133)
- Melt viscosity: 450 Pa·s (1000 s⁻¹/260 °C, ISO 11443-A)
- Molding shrinkage (parallel/normal): 0.5–0.7% (150×105×3 mm³, 260 °C/MT 80 °C, ISO 2577)
Mechanical properties (23 °C/50 % r. h.)
- Tensile modulus: 2400 MPa (1 mm/min, ISO 527-1, -2)
- Yield stress: 63 MPa (50 mm/min, ISO 527-1, -2)
- Yield strain: 5% (50 mm/min, ISO 527-1, -2)
- Izod notched impact strength (23 °C): 45 kJ/m² (ISO 180/A)
- Izod notched impact strength (-30 °C): 15 kJ/m² (ISO 180/A)
Thermal properties
- Temperature of deflection under load:
- 114 °C (1.80 MPa, ISO 75-1, -2)
- 126 °C (0.45 MPa, ISO 75-1, -2)
- Vicat softening temperature:
- 134 °C (50 N, 50 °C/h, ISO 306)
- 136 °C (50 N, 120 °C/h, ISO 306)
- Coefficient of linear thermal expansion (parallel/normal): 0.68×10⁻⁴/K (23 to 55 °C, ISO 11359-1, -2)
- Burning behavior:
- UL 94 V-0 (1.5 mm, UL 94)
- UL 94 5VB (2.0 mm, UL 94)
- UL 94 5VA (3.0 mm, UL 94)
Electrical properties (23 °C/50 % r. h.)
- Relative permittivity:
- 3.2 (100 Hz, IEC 60250)
- 3.1 (1 MHz, IEC 60250)
- Dissipation factor:
- 20 × 10⁻⁴ (100 Hz, IEC 60250)
- 85 × 10⁻⁴ (1 MHz, IEC 60250)
- Volume resistivity: 1 × 10¹⁵ Ohm·m (IEC 62631-3-1)
- Surface resistivity: 1 × 10¹⁷ Ohm (IEC 62631-3-2)
- Electrical strength: 35 kV/mm (1 mm, IEC 60243-1)
- Comparative Tracking Index (CTI): 350 (Solution A, IEC 60112)
Other properties (23 °C)
- Water absorption (saturation): 0.5% (Water at 23 °C, ISO 62)
- Water absorption (equilibrium): 0.2% (23 °C, 50% r.h., ISO 62)
- Density: 1190 kg/m³ (ISO 1183-1)
Process Guide
- Injection molding melt temperature: 260 °C (ISO 294)
- Mold temperature: 80 °C (ISO 294)
- Injection velocity: 240 mm/s (ISO 294)
- Recommended melt temperatures: 240–280 °C
- Drying temperature and time: 80 °C for 4 h (max. 0.02% moisture content)
Use & Applications
- Injection molding
- Supporting material for energized parts
Features & Benefits
Superior Flame Retardancy
Bayblend FR1514 achieves UL 94 V-0 compliance at just 1.5 mm thickness, reducing fire risks in electronics and electrical enclosures without compromising design flexibility.
High Heat Resistance
With a Vicat softening temperature of 136°C and deflection resistance up to 126°C (0.45 MPa), this material withstands demanding thermal environments, ensuring long-term reliability.
Tough & Impact-Resistant
It boasts 45 kJ/m² notched impact strength at 23°C (ISO 180/A), preventing cracks or breaks in rugged applications like power tools or automotive housings.