Covestro Bayblend® FR3000 HI PC/ABS

covestro bayblend pc abs blend

Bayblend® FR3000 HI PC/ABS Resin

Bayblend FR3000 HI is a flame-retardant PC+ABS resin, delivering UL 94 V-0 certification at 1.5 mm thickness. It excels in impact resistance, chemical stability, and thermal performance (Vicat 97°C). Ideal for demanding electrical/automotive components where safety and durability are critical.

Download PDF

Typical property data

Physical Properties (Rheological)
  • Melt volume-flow rate: 20 cm³/10 min (240 °C/5 kg, ISO 1133)
  • Melt viscosity: 185 Pa·s (1000 s⁻¹, 260 °C, ISO 11443-A)
  • Molding shrinkage:
    • Parallel: 0.5–0.7% (240 °C, ISO 2577)
    • Normal: 0.5–0.7% (240 °C, ISO 2577)
Mechanical Properties (23 °C/50% r.h.)
  • Tensile modulus: 2700 MPa (1 mm/min, ISO 527-1,-2)
  • Yield stress: 60 MPa (50 mm/min, ISO 527-1,-2)
  • Yield strain: 4.0% (50 mm/min, ISO 527-1,-2)
  • Izod notched impact strength:
    • 23 °C: 35 kJ/m² (ISO 180/A)
    • -30 °C: 10 kJ/m² (ISO 180/A)
Thermal Properties
  • Heat deflection temperature (HDT):
    • 1.80 MPa: 82 °C (ISO 75-1,-2)
    • 0.45 MPa: 92 °C (ISO 75-1,-2)
  • Vicat softening temperature:
    • 50 N, 50 °C/h: 95 °C (ISO 306)
    • 50 N, 120 °C/h: 97 °C (ISO 306)
  • Coefficient of linear thermal expansion:
    • Parallel: 7.6×10−57.6 \times 10^{-5} K⁻¹ (23–55 °C, ISO 11359-1,-2)
    • Normal: 8.0×10−58.0 \times 10^{-5} K⁻¹ (23–55 °C, ISO 11359-1,-2)
  • Flammability ratings:
    • UL 94 V-0 (1.5 mm)
    • UL 94 5VB (2.0 mm)
    • UL 94 5VA (3.0 mm)
Electrical Properties (23 °C/50% r.h.)
  • Relative permittivity:
    • 100 Hz: 3.2 (IEC 60250)
    • 1 MHz: 3.1 (IEC 60250)
  • Dissipation factor:
    • 100 Hz: 5.0×10−35.0 \times 10^{-3} (IEC 60250)
    • 1 MHz: 6.0×10−36.0 \times 10^{-3} (IEC 60250)
  • Volume resistivity: 1×1014 Ω⋅m1 \times 10^{14}\, \Omega·m (IEC 62631-3-1)
  • Surface resistivity: 1×1016 Ω1 \times 10^{16}\, \Omega (IEC 62631-3-2)
  • Electrical strength: 35 kV/mm (IEC 60243-1)
  • Comparative tracking index (CTI): 350 (Solution A, IEC 60112)
Other Properties (23 °C)
  • Density: 1180 kg/m³ (ISO 1183-1)
  • Water absorption:
    • Saturation value: 0.5% (ISO 62)
    • Equilibrium value: 0.2% (23 °C, 50% r.h., ISO 62)
Processing Guide

Injection molding conditions:

  • Melt temperature: 240–270 °C (Standard: 260 °C, ISO 294)
  • Mold temperature: 60–80 °C (ISO 294)
  • Hold pressure (% of injection pressure): 50–75%
  • Drying conditions (Dry air dryer):
    • Temperature: 80 °C
    • Time: 4 hours
    • Max moisture content: ≤ 0.02%

Use & Applications

  • Electrical: Circuit breakers, switchgear, connector housings
  • Automotive: Battery covers, sensor housings, interior trim
  • Consumer Electronics: Power tool casings, charger enclosures
  • Industrial: Control panels, safety equipment housings
covestro bayblend pc abs blend

Features & Benefits

Uncompromised Flame Safety

It achieves UL 94 V-0 at just 1.5 mm thickness, preventing flame spread in high-risk environments like electronics housings. Ensures compliance with strict safety regulations.

Enhanced Durability & Resistance

Superior impact strength (35 kJ/m²) and chemical resistance reduce stress cracking and part failure in harsh industrial settings. Lowers maintenance costs.

Reliable Thermal Stability

It withstands 97°C (Vicat B120), ensuring dimensional stability in heat-exposed applications like automotive interiors or power tools.