Plastic Granules
Bayblend® FR3002 PC/ABS Resin Flame-retardant
Bayblend FR3002 is a flame-retardant thermoplastic blend of (PC+ABS). With UL 94 V-0 certification at just 1.0 mm thickness and a Vicat softening temperature of 99°C, it excels in thin-wall designs like electronics housings while ensuring superior fire resistance.
Download PDF
ISO TDS
Typical property data
Physical Properties (Rheological)
- Melt volume-flow rate: 19 cm³/10 min (240 °C/5 kg, ISO 1133)
- Melt viscosity: 190 Pa·s (1000 s⁻¹/260 °C, ISO 11443-A)
- Molding shrinkage (parallel/normal): 0.5–0.7% (240 °C/MT 80 °C, ISO 2577)
Mechanical Properties (23 °C/50% r.h.)
- Tensile modulus: 2700 MPa (1 mm/min, ISO 527-1,-2)
- Yield stress: 60 MPa (50 mm/min, ISO 527-1,-2)
- Yield strain: 4.0% (50 mm/min, ISO 527-1,-2)
- Flexural modulus: 2600 MPa (2 mm/min, ISO 178)
- Flexural strength: 98 MPa (2 mm/min, ISO 178)
- Izod notched impact strength: 30 kJ/m² (23 °C, ISO 180/A)
Thermal Properties
- Deflection temperature under load:
- 84 °C (1.80 MPa, ISO 75-1,-2)
- 92 °C (0.45 MPa, ISO 75-1,-2)
- Vicat softening temperature:
- 97 °C (50 N, 50 °C/h, ISO 306)
- 99 °C (50 N, 120 °C/h, ISO 306)
- Coefficient of linear thermal expansion:
- Parallel: 0.76×10−40.76 \times 10^{-4}0.76×10−4 /K (23–55 °C, ISO 11359-1,-2)
- Normal: 0.80×10−40.80 \times 10^{-4}0.80×10−4 /K (23–55 °C, ISO 11359-1,-2)
- Burning behavior:
- UL 94 V-0 (1.0 mm, UL 94)
- UL 94 5VB (1.8 mm, UL 94)
Electrical Properties (23 °C/50% r.h.)
- Relative permittivity:
- 3.2 (100 Hz, IEC 60250)
- 3.1 (1 MHz, IEC 60250)
- Dissipation factor:
- 5.0×10−35.0 \times 10^{-3}5.0×10−3 (100 Hz, IEC 60250)
- 6.0×10−36.0 \times 10^{-3}6.0×10−3 (1 MHz, IEC 60250)
- Volume resistivity: 1×10141 \times 10^{14}1×1014 Ohm·m (IEC 62631-3-1)
- Surface resistivity: 1×10161 \times 10^{16}1×1016 Ohm (IEC 62631-3-2)
- Electrical strength: 35 kV/mm (1 mm, IEC 60243-1)
- Comparative tracking index (CTI): 350 (Solution A, IEC 60112)
Other Properties (23 °C)
- Water absorption (saturation): 0.5% (Water at 23 °C, ISO 62)
- Water absorption (equilibrium): 0.2% (23 °C/50% r.h., ISO 62)
- Density: 1180 kg/m³ (ISO 1183-1)
Process Guide
- Melt temperature: 240–270 °C (ISO 294)
- Mold temperature: 60–80 °C (ISO 294)
- Injection velocity: 240 mm/s (ISO 294)
- Hold pressure: 50–75% of injection pressure
- Plastic back pressure: 50–150 bar
- Dry air drying temperature: 80 °C
- Drying time: 4 hours
- Maximum moisture content: ≤ 0.02%
Use & Applications
- Electronics: Notebook housings, charger plugs, and ultra-slim device components.
- Thin-Wall Parts: Battery covers, connector housings (<1.5 mm).
- Safety-Focused Parts: Automotive interior trims, industrial enclosures requiring flame resistance.
Features & Benefits
Reliable Flame Resistance
Bayblend® FR3002 achieves UL 94 V-0 compliance at 1.0 mm, reducing fire risks in compact electronics. Ideal for notebooks and chargers where space is limited but safety is non-negotiable.
High Flow for Thin Walls
With a melt flow rate of 19 cm³/10 min (240°C/5 kg), it fills intricate molds effortlessly. Enables lightweight, complex parts like slim laptop bezels without compromising structural integrity.
Robust Impact & Heat Resistance
It delivers 30 kJ/m² notched impact strength and 92°C HDT (0.45 MPa). Protects devices from drops and thermal stress in demanding environments like automotive interiors.