Plastic Granules
Bayblend® FR3008 RE PC/ABS Resin
Bayblend FR3008 RE is a flame-retardant PC/ABS blend offering high impact strength, excellent thermal stability (HDT 85°C), and UL 94 V-0 recognition at 1.5mm for superior safety in demanding applications.
Download PDF
ISO TDS
Typical property data
Physical Properties (Rheological)
- Melt volume-flow rate: 13 cm³/10 min (ISO 1133, at 240 °C/5 kg)
- Melt viscosity: 195 Pa·s (ISO 11443-A, at 1000 s⁻¹/260 °C)
- Molding shrinkage (parallel/normal): 0.5–0.7% (ISO 2577, 150×105×3 mm³, 240 °C/MT 80 °C)
Mechanical Properties (23 °C/50 % r. h.)
- Tensile modulus: 2800 MPa (ISO 527-1,-2, 1 mm/min)
- Yield stress: 60 MPa (ISO 527-1,-2, 50 mm/min)
- Yield strain: 4.0% (ISO 527-1,-2, 50 mm/min)
- Flexural modulus: 2700 MPa (ISO 178, 2 mm/min)
- Flexural strength: 98 MPa (ISO 178, 2 mm/min)
- Izod notched impact strength:
- 23 °C: 30 kJ/m² (ISO 180/A)
- -30 °C: 10 kJ/m² (ISO 180/A)
Thermal Properties
- Deflection temperature under load:
- 1.80 MPa: 85 °C (ISO 75-1,-2)
- 0.45 MPa: 95 °C (ISO 75-1,-2)
- Vicat softening temperature:
- 50 N, 50 °C/h: 101 °C (ISO 306)
- 50 N, 120 °C/h: 103 °C (ISO 306)
- Coefficient of linear thermal expansion:
- Parallel: 0.76×10⁻⁴/K (ISO 11359-1,-2, 23–55 °C)
- Normal: 0.8×10⁻⁴/K (ISO 11359-1,-2, 23–55 °C)
- Burning behavior:
- UL 94 (1.5 mm): V-0 (UL 94)
- UL 94-5V (2.0 mm): 5VB (UL 94)
- Glow wire temperature (GWFI): 960 °C (2.0 mm, IEC 60695-2-12)
- Oxygen index: 32% (ISO 4589-2, Method A)
Electrical Properties (23 °C/50 % r. h.)
- Relative permittivity:
- 100 Hz: 3.2 (IEC 60250)
- 1 MHz: 3.1 (IEC 60250)
- Dissipation factor:
- 100 Hz: 50×10⁻⁴ (IEC 60250)
- 1 MHz: 70×10⁻⁴ (IEC 60250)
- Volume resistivity: 1×10¹⁴ Ω·m (IEC 62631-3-1)
- Surface resistivity: 1×10¹⁶ Ω (IEC 62631-3-2)
- Electrical strength: 30 kV/mm (IEC 60243-1)
- Comparative tracking index (CTI): 300 (IEC 60112, Solution A)
Other Properties (23 °C)
- Water absorption (saturation value): 0.5% (ISO 62, water at 23 °C)
- Water absorption (equilibrium value): 0.2% (ISO 62, 23 °C, 50 % r. h.)
- Density: 1180 kg/m³ (ISO 1183-1)
Processing Guide
- Melt temperature: 240–270 °C (ISO 294)
- Mold temperature: 60–90 °C (ISO 294)
- Injection velocity: 240 mm/s (ISO 294)
- Moisture content (max.): ≤ 0.02%
- Drying conditions:
- Dry air drying temperature: 80 °C
- Drying time: 4 hours
Use & Applications
- Electrical Enclosures and Housings (e.g., power strips, connectors, control units)
- Consumer Electronics Components (e.g., internal chassis, battery holders, plugs)
- Automotive Interior Parts (non-critical, non-food contact components)
- Business Machine Housings (e.g., printers, scanners, data storage devices)
- Components Requiring a High Glow-Wire Rating
Features & Benefits
Superior Flame Retardancy & Safety
It achieves a UL 94 V-0 rating at just 1.5mm thickness, ensuring critical components meet stringent international safety standards and reduce fire risks in enclosed spaces.
Exceptional Impact Strength & Durability
It offers high notched impact resistance, providing excellent toughness and structural integrity to prevent cracking or failure from physical shocks or drops during use.
High Thermal & Electrical Performance
It features a high glow-wire temperature (960°C) and comparative tracking index (CTI 300), ideal for electrical housings that must resist heat and prevent electrical failure.