Plastic Granules
Bayblend® FR3008 PC/ABS Resin
Covestro PC+ABS Bayblend FR3008 is a flame-retardant, non-reinforced blend engineered for demanding applications. With UL 94 V-0 certification at 1.5 mm, a Vicat B 120 temperature of 103°C, and exceptional chemical resistance, it ensures safety and durability in high-heat environments. Ideal for electronics and automotive components.
Download PDF
ISO TDS
Typical property data
Physical Properties (Rheological)
- Melt volume-flow rate (240 °C/5 kg): 13 cm³/10 min (ISO 1133)
- Melt viscosity (1000 s⁻¹, 260 °C): 195 Pa·s (ISO 11443-A)
- Molding shrinkage (parallel): 0.5–0.7 % (150x105x3 mm³, 240 °C/MT 80 °C, ISO 2577)
- Molding shrinkage (normal): 0.5–0.7 % (ISO 2577)
Mechanical properties (23 °C/50 % r. h.)
- Tensile modulus: 2800 MPa (1 mm/min, ISO 527-1,-2)
- Yield stress: 60 MPa (50 mm/min, ISO 527-1,-2)
- Yield strain: 4.0 % (50 mm/min, ISO 527-1,-2)
- Stress at break: 50 MPa (50 mm/min, ISO 527-1,-2)
- Flexural modulus: 2700 MPa (2 mm/min, ISO 178)
- Flexural strength: 98 MPa (2 mm/min, ISO 178)
- Izod notched impact strength (23 °C): 30 kJ/m² (ISO 180/A)
- Izod notched impact strength (-30 °C): 10 kJ/m² (ISO 180/A)
Thermal properties
- Temperature of deflection under load (1.80 MPa): 85 °C (ISO 75-1,-2)
- Temperature of deflection under load (0.45 MPa): 95 °C (ISO 75-1,-2)
- Vicat softening temperature (50 N; 120 °C/h): 103 °C (ISO 306)
- Burning behavior (UL 94, 1.5 mm): UL 94 V-0 (UL Recognition)
- Glow wire test (GWFI): 960 °C (2.0 mm, IEC 60695-2-12)
Electrical properties (23 °C/50 % r. h.)
- Relative permittivity (100 Hz): 3.2 (IEC 60250)
- Relative permittivity (1 MHz): 3.1 (IEC 60250)
- Dissipation factor (100 Hz): 50 x 10⁻⁴ (IEC 60250)
- Volume resistivity: 1E14 Ohm·m (IEC 62631-3-1)
- Electrical strength: 30 kV/mm (1 mm, IEC 60243-1)
Other properties (23 °C)
- Water absorption (saturation value): 0.5 % (Water at 23 °C, ISO 62)
- Density: 1180 kg/m³ (ISO 1183-1)
Process Guide
- Melt temperature: 240–270 °C (ISO 294)
- Mold temperature: 60–90 °C (ISO 294)
- Moisture content max.: ≤ 0.02 %
- Dry air drying temperature: 80 °C
- Dry air drying time: 4 hours
Use & Applications
- Electrical & Electronics: Circuit breakers, server housings, and connectors requiring flame resistance.
- Automotive Interiors: Dashboard components, control panels, and vents needing heat tolerance.
- Consumer Electronics: Power-tool casings, laptop bases, and LED housings with strict safety standards.
- Industrial Equipment: Enclosures for machinery exposed to chemicals or high temperatures.
Features & Benefits
Superior Flame Retardancy
Bayblend® FR3008 achieves UL 94 V-0 certification at just 1.5 mm thickness and resists ignition up to 960°C (GWFI). This reduces fire risks in electronics and meets strict safety regulations without costly additives.
Enhanced Thermal Stability
With an HDT/A of ≥85°C and Vicat softening at 103°C, this PC+ABS blend maintains structural integrity under heat. Perfect for automotive dashboards or power-tool housings exposed to high operating temperatures.
Reliable Processability
Optimized melt flow (13 cm³/10 min) and low molding shrinkage (0.5–0.7%) ensure consistent injection molding. Minimizes warping and rejects in high-volume production of complex parts like connectors or enclosures.