Covestro Bayblend® FR3013 PC/ABS

covestro bayblend pc abs blend

Bayblend® FR3013 PC/ABS Resin

Bayblend FR3013 is an easy-flowing, flame-retardant (PC+ABS) blend engineered for demanding injection-molded IT components. With high impact resistance and a Vicat softening temperature of 95°C, it ensures safety, durability, and efficiency in electronics enclosures and office hardware.

Download PDF

Typical property data

Physical Properties (Rheological)
  • Melt Volume-Flow Rate (240 °C/5 kg): 26 cm³/10 min (ISO 1133)
  • Melt Viscosity (1000 s⁻¹, 240 °C): 155 Pa·s (ISO 11443-A)
  • Molding Shrinkage (Normal, 60x60x2 mm³): 0.4–0.6% (ISO 294-4)
Mechanical properties (23 °C/50 % r. h.)
  • Tensile Modulus (1 mm/min): 2650 MPa (ISO 527-1,-2)
  • Yield Stress (50 mm/min): 61 MPa (ISO 527-1,-2)
  • Yield Strain (50 mm/min): 4% (ISO 527-1,-2)
  • Flexural Modulus (2 mm/min): 2600 MPa (ISO 178)
  • Flexural Strength (2 mm/min): 93 MPa (ISO 178)
  • Izod Notched Impact Strength (23 °C): 34 kJ/m² (ISO 180/A)
  • Izod Notched Impact Strength (-30 °C): 8 kJ/m² (ISO 180/A)
Thermal properties
  • Deflection Temperature Under Load (1.80 MPa): 78 °C (ISO 75-1,-2)
  • Deflection Temperature Under Load (0.45 MPa): 86 °C (ISO 75-1,-2)
  • Vicat Softening Temperature (50 N; 120 °C/h): 95 °C (ISO 306)
  • Coefficient of Linear Thermal Expansion (23–55 °C, Parallel): 0.75 × 10⁻⁴/K (ISO 11359-1,-2)
  • Burning Behavior (UL 94, 1.5 mm): V-0 (Classified)
  • Oxygen Index: 31% (ISO 4589-2)
Electrical properties (23 °C/50 % r. h.)
  • Volume Resistivity: 2.0×10162.0 \times 10^{16} Ohm·m (IEC 62631-3-1)
  • Surface Resistivity: 5.0×10175.0 \times 10^{17} Ohm (IEC 62631-3-2)
Other properties (23 °C)
  • Density: 1190 kg/m³ (ISO 1183-1)
Process Guide
  • Injection Molding Melt Temperature: 240–270 °C (ISO 294)
  • Mold Temperature: 60–80 °C (ISO 294)
  • Injection Velocity: 240 mm/s (ISO 294)
  • Drying Temperature: 80 °C
  • Drying Time: 4 hours
  • Maximum Moisture Content: ≤0.02%

Use & Applications

  • Information Technology (IT): Laptop/tablet housings; Server enclosures; Printer/scanner components; Electrical connectors and sockets; Office equipment casings.
covestro bayblend pc abs blend

Features & Benefits

Top-Tier Flame Retardancy

It achieves UL94 V-0 and 5VB ratings at 1.5mm thickness, preventing fire spread in IT housings and electrical enclosures—critical for compliance and user safety.

High Impact Strength

It delivers 34 kJ/m² notched Izod impact resistance (23°C), protecting devices like laptops and printers from drops, vibrations, and rough handling.

Easy-Flowing Processing

Melt flow rate of 26 cm³/10min ensures fast, precise mold filling—ideal for complex IT parts like thin-wall connectors, reducing cycle times and waste.