Plastic Granules
Bayblend® FR3020 W BBS910 PC/ABS Resin
Bayblend FR3020 W BBS910 is a flame-retardant, mineral-filled PC/ABS blend offering high impact strength, excellent UV stability, and a UL 94 V-0 rating at 0.6mm for superior safety in thin-wall components.
Download PDF
ISO TDS
Typical property data
Physical Properties (Rheological)
- Melt volume-flow rate (MVR): 24 cm³/10 min at 260 °C/5 kg (ISO 1133)
- Melt viscosity: 250 Pa·s at 1000 s⁻¹/260 °C (ISO 11443-A)
Mechanical properties (23 °C/50 % r. h.)
- Tensile modulus: 3200 MPa (ISO 527-1, -2)
- Yield stress: 67 MPa (ISO 527-1, -2)
- Yield strain: 4% (ISO 527-1, -2)
- Stress at break: 51 MPa (ISO 527-1, -2)
- Strain at break: >50% (ISO 527-1, -2)
- Izod notched impact strength (23 °C): 12 kJ/m² (ISO 180/A)
- Izod notched impact strength (-30 °C): 8 kJ/m² (ISO 180/A)
Thermal properties
- Vicat softening temperature: 102 °C under 50 N, 120 °C/h (ISO 306)
- Flame retardancy: UL 94 V-0 (at 0.6 mm thickness)
Process Guide
- Injection molding – Melt temperature: 260 °C (ISO 294)
- Injection molding – Mold temperature: 80 °C (ISO 294)
- Injection molding – Injection velocity: 240 mm/s (ISO 294)
Use & Applications
- Injection Molding
- Electrical Enclosures
- Consumer Electronics
- Automotive Components
- Connectors and Sockets
Features & Benefits
Superior Flame Retardancy & Safety
This material achieves a UL 94 V-0 rating at just 0.6mm thickness and features low smoke density, enhancing evacuation time and safety in critical electrical applications.
Excellent Impact Strength & Durability
Its impact-modified formulation provides high notched impact strength, ensuring components can withstand physical shocks and rough handling throughout their lifecycle.
High Thermal Stability & Processability
With a Vicat softening temperature of 102°C and balanced flow characteristics, it maintains dimensional stability under heat and is easy to process via injection molding.