Covestro Bayblend® FR3110 TV PC/ABS

covestro bayblend pc abs blend

Bayblend® FR3110 TV PC/ABS Resin

Bayblend® FR3110 TV is a flame-retardant, easy-flow PC/ABS blend offering high heat resistance (Vicat 110°C) and a UL94 V-0 rating at just 1.5mm for demanding electrical and electronic applications.

Associated Documents

ISO TDS

Typical property data

Physical Properties (Rheological)
  • Density: 1.20 g/cm³ (ISO 1183)
  • Melt Volume Rate (MVR): 17 cm³/10 min (260 °C/5.0 kg, ISO 1133)
Mechanical properties (23 °C/50 % r. h.)
  • Tensile Modulus: 2300 MPa (ISO 527-1/-2)
  • Tensile Stress at Yield: 50 MPa (ISO 527-1/-2)
  • Tensile Strain at Yield: 5.0% (ISO 527-1/-2)
  • Charpy Notched Impact Strength: 35 kJ/m² (23 °C, ISO 179/1eA)
Thermal properties
  • Heat Deflection Temperature (HDT): 80 °C (1.80 MPa, ISO 75-1/-2)
  • Vicat Softening Temperature: 110 °C (50 N, ISO 306)
  • Relative Temperature Index (RTI): 80 °C (UL 746B)
Electrical properties (23 °C/50 % r. h.)
  • Comparative Tracking Index (CTI): 250 V (IEC 60112)
  • Volume Resistivity: 10¹⁵ Ω·cm (IEC 60093)
  • Dielectric Strength: 23 kV/mm (3.2 mm, IEC 60243-1)
Other properties (23 °C)
  • Flammability Rating: UL 94 V-0 (0.75 mm thickness)
  • Glow Wire Flammability Index (GWFI): 960 °C (IEC 60695-2-12)
  • Glow Wire Ignition Temperature (GWIT): 775 °C (IEC 60695-2-13)
Process Guide
  • Drying Temperature: 100–120 °C
  • Drying Time: 2–4 hours
  • Melt Temperature: 250–270 °C
  • Mold Temperature: 80–100 °C
  • Injection Speed: Medium to high

Features & Benefits

Superior Flame Retardancy & Safety

It achieves a UL94 V-0 rating at a thin 1.5mm, ensuring critical fire safety and compliance for compact, modern electronic device housings and components.

Excellent Flow & Processability

Its high melt flow rate ensures easy filling of complex, thin-walled molds, reducing cycle times and improving production efficiency for high-volume manufacturing.

Enhanced Thermal Resistance

With a Vicat softening temperature of 110°C, it provides increased heat resistance, ensuring dimensional stability in environments prone to warmth, like inside appliances.

covestro bayblend pc abs blend

Use & Applications

  • Electrical enclosures and housings (e.g., power strips, connectors, circuit breakers)
  • Consumer electronics components (e.g., laptop internal supports, charger housings)
  • Automotive interior parts requiring flame retardancy
  • Housing for small domestic appliances