Plastic Granules
Bayblend® PC/ABS Resin
Bayblend® FR3210 TV is a flame-retardant PC+ABS blend offering excellent flow, a high Vicat softening temperature of 93°C, and superior surface quality, certified UL 94 V-0 at just 1.2 mm.
Associated Documents
ISO TDS
Typical property data
Physical Properties (Rheological)
- Melt Volume-Flow Rate (MVR): 38 cm³/10 min (240 °C, 5 kg) [ISO 1133]
- Melt Viscosity: 135 Pa·s (1000 s⁻¹, 260 °C) [ISO 11443-A]
- Molding Shrinkage (Parallel and Normal): 0.5%–0.7% (150×105×3 mm³; 240 °C; MT 80 °C) [ISO 2577]
Mechanical properties (23 °C/50 % r. h.)
- Tensile Modulus: 2700 MPa (1 mm/min) [ISO 527-1, -2]
- Yield Stress: 60 MPa (50 mm/min) [ISO 527-1, -2]
- Yield Strain: 3.5% (50 mm/min) [ISO 527-1, -2]
- Stress at Break: 45 MPa (50 mm/min) [ISO 527-1, -2]
- Strain at Break: >30% (50 mm/min) [ISO 527-1, -2]
- Izod Notched Impact Strength: 30 kJ/m² (23 °C) [ISO 180/A]
Thermal properties
- Temperature of Deflection Under Load (HDT):
- 76 °C (1.80 MPa) [ISO 75-1, -2]
- 85 °C (0.45 MPa) [ISO 75-1, -2]
- Vicat Softening Temperature:
- 91 °C (50 N, 50 °C/h) [ISO 306]
- 93 °C (50 N, 120 °C/h) [ISO 306]
- Coefficient of Linear Thermal Expansion:
- 0.75×10⁻⁴/K (Parallel and Normal, 23–55 °C) [ISO 11359-1, -2]
- Burning Behavior: UL 94 V-0 at 1.2 mm and 1.5 mm thickness [UL 94]
Other properties (23 °C)
- Water Absorption (Saturation): 0.5% (Water at 23 °C) [ISO 62]
- Water Absorption (Equilibrium): 0.2% (23 °C, 50% r.h.) [ISO 62]
- Density: 1180 kg/m³ [ISO 1183-1]
Process Guide
- Injection Molding Melt Temperature: 240–270 °C (Standard: 250 °C) [ISO 294]
- Mold Temperature: 60–80 °C [ISO 294]
- Injection Velocity: 240 mm/s [ISO 294]
- Drying Conditions:
- Temperature: 80 °C
- Time: 4 hours
- Moisture Content (Max): ≤0.02%
Features & Benefits
Superior Flame Retardancy & Safety
This material achieves a UL 94 V-0 rating at a thin 1.2 mm, enabling the design of safer, lighter, and more compact components for electronics and enclosures without compromising safety.
Excellent Flow for Complex Parts
With its high melt flow rate, it fills intricate molds easily, reducing injection pressure and cycle times. This means higher productivity and fewer rejects for complex, thin-walled designs.
Enhanced Heat Resistance & Stability
A Vicat softening temperature of 93°C ensures dimensional stability and performance in elevated temperature environments, ideal for components near heat sources in electronic devices.
Use & Applications
- Electrical enclosures and housings
- Connectors and sockets
- Consumer electronics components
- Charger housings
- Automotive interior components