Plastic Granules
Bayblend® M850 XF PC/ABS Resin
Bayblend M850 XF is an easy-flow PC/ABS blend engineered for medical devices. It offers high heat resistance (Vicat 131°C) and is designed to meet specific biological safety requirements per ISO 10993-1.
Associated Documents
ISO TDS
Typical property data
Physical Properties (Rheological)
- Melt volume-flow rate: 25 cm³/10 min (260 °C/5 kg, ISO 1133)
- Melt viscosity: 210 Pa·s (1000 s⁻¹/260 °C, ISO 11443-A)
- Molding shrinkage (parallel): 0.55–0.75% (ISO 2577)
- Molding shrinkage (normal): 0.55–0.75% (ISO 2577)
Mechanical Properties (23 °C/50% r.h.)
- Tensile modulus: 2500 MPa (1 mm/min, ISO 527-1,-2)
- Yield stress: 62 MPa (50 mm/min, ISO 527-1,-2)
- Yield strain: 4.9% (50 mm/min, ISO 527-1,-2)
- Stress at break: 53 MPa (50 mm/min, ISO 527-1,-2)
- Strain at break: >50% (50 mm/min, ISO 527-1,-2)
- Izod notched impact strength (23 °C): 48 kJ/m² (ISO 180/A)
- Izod notched impact strength (-30 °C): 15 kJ/m² (ISO 180/A)
Thermal Properties
- Temperature of deflection under load (1.80 MPa): 109 °C (ISO 75-1,-2)
- Temperature of deflection under load (0.45 MPa): 127 °C (ISO 75-1,-2)
- Vicat softening temperature: 129–131 °C (50 N; ISO 306)
- Coefficient of linear thermal expansion (parallel/normal): 0.7 × 10⁻⁴/K (23–55 °C, ISO 11359-1,-2)
- Burning behavior: UL 94 HB (0.85 mm, UL 94)
Electrical Properties (23 °C/50% r.h.)
- Relative permittivity: 2.9 (100 Hz and 1 MHz, IEC 60250)
- Dissipation factor: 30 × 10⁻⁴ (100 Hz) / 90 × 10⁻⁴ (1 MHz, IEC 60250)
- Volume resistivity: 1 × 10¹⁴ Ohm·m (IEC 62631-3-1)
- Surface resistivity: 1 × 10¹⁷ Ohm (IEC 62631-3-2)
- Electrical strength: 35 kV/mm (1 mm, IEC 60243-1)
- Comparative tracking index (CTI): 250 (Solution A, IEC 60112)
Other Properties (23 °C)
- Water absorption (saturation): 0.7% (Water at 23 °C, ISO 62)
- Water absorption (equilibrium): 0.2% (23 °C/50% r.h., ISO 62)
- Density: 1140 kg/m³ (ISO 1183-1)
Processing and Drying Conditions
- Injection molding melt temperature: 260 °C (ISO 294)
- Injection molding mold temperature: 80 °C (ISO 294)
- Drying temperature: 95–110 °C (dry air drying)
- Drying time: 4 hours
- Moisture content (max): ≤0.02%
Use & Application
- Injection Molding of critical medical device components.
- Medical Devices: Housings for diagnostic equipment; Components for drug delivery devices; Handles and enclosures for surgical tools; edical instrument casings.
Features & Benefits
1. Excellent Flow for Complex Parts
Its high melt flow rate ensures easy filling of intricate, thin-walled molds, reducing cycle times and minimizing internal stresses for superior part quality and productivity.
2. Superior Impact Strength & Durability
This grade provides outstanding toughness, even at room temperature, ensuring medical device housings and components can withstand impact during use, assembly, and transportation.
3. High Heat & Thermal Resistance
With a Vicat softening temperature of 131°C, it reliably withstands repeated heat-based sterilization cycles, such as autoclaving, ensuring device integrity and longevity.