Covestro Makrolon® 2207 PC Resin

covestro makrolon® pc resin 25kg package

Makrolon® 2207 Polycarbonate PC Resin Injection molding Grade

Makrolon® 2207 is a general-purpose, low-viscosity polycarbonate resin from Covestro. Engineered for injection molding, it offers excellent clarity, dimensional stability, and strength—ideal for demanding industrial applications.

Associated Documents

ISO TDS
UL Product iQ

Typical property data

Physical Properties (Rheological)
  • Melt Volume-Flow Rate: 34 cm³/10 min (300 °C/1.2 kg, ISO 1133)
  • Melt Mass-Flow Rate: 37 g/10 min (300 °C/1.2 kg, ISO 1133)
  • Molding Shrinkage (Parallel/Normal): 0.5–0.7% (ISO 2577)
Mechanical Properties (23 °C/50 % r. h.)
  • Tensile Modulus: 2400 MPa (1 mm/min, ISO 527-1,-2)
  • Yield Stress: 65 MPa (50 mm/min, ISO 527-1,-2)
  • Yield Strain: 6.0% (50 mm/min, ISO 527-1,-2)
  • Flexural Modulus: 2350 MPa (2 mm/min, ISO 178)
  • Flexural Strength: 98 MPa (2 mm/min, ISO 178)
  • Charpy Notched Impact Strength: 55 kJ/m² (23 °C, ISO 21305/ISO 179/1eA)
  • Puncture Energy: 55 J (23 °C, ISO 6603-2)
Thermal Properties
  • Glass Transition Temperature: 144 °C (ISO 11357-1,-2)
  • Temperature of Deflection Under Load:
    • 123 °C (1.80 MPa, ISO 75-1,-2)
    • 136 °C (0.45 MPa, ISO 75-1,-2)
  • Vicat Softening Temperature: 143 °C (50 N, 50 °C/h, ISO 306)
  • Burning Behavior:
    • V-2 (0.75 mm, UL 94)
    • HB (2.9 mm, UL 94)
Electrical Properties (23 °C/50 % r. h.)
  • Relative Permittivity: 3.1 (100 Hz, IEC 60250)
  • Dissipation Factor: 5×10−45 \times 10^{-4} (100 Hz, IEC 60250)
  • Volume Resistivity: 1×10141 \times 10^{14} Ohm·m (IEC 62631-3-1)
  • Electrical Strength: 34 kV/mm (1 mm, IEC 60243-1)
Other Properties (23 °C)
  • Water Absorption (Saturation Value): 0.30% (ISO 62)
  • Density: 1190 kg/m³ (ISO 1183-1)
  • Refractive Index: 1.586 (ISO 489)
Processing and Drying Conditions
  • Melt Temperature: 280–320 °C (Recommended: 300 °C, ISO 294)
  • Mold Temperature: 80–120 °C (ISO 294)
  • Drying Temperature: 120 °C
  • Drying Time: 2–3 hours
  • Moisture Content (Max): ≤ 0.02%

Features & Benefits

Effortless Injection Molding

Makrolon 2207’s low viscosity (MVR 35 cm³/10 min) ensures smooth flow into intricate molds, reducing cycle times and minimizing defects like air traps—ideal for high-volume precision parts.

Toughness in Extreme Conditions

It boasts Charpy notched impact strength of 55 kJ/m² at 23°C and retains performance at -30°C, making it perfect for automotive or outdoor gear exposed to impacts and temperature swings.

Heat & Flame Resistance

With a heat deflection temperature of 123°C (1.8 MPa) and UL 94 V-2 flame rating (0.75 mm), it ensures safety and stability in electronics and enclosures near heat sources.

covestro makrolon® pc resin 25kg package

Use & Applications

  • Durable enclosures: Electrical housings, power tools, and control panels.
  • Automotive parts: Interior trim, light covers, and connectors.
  • Consumer goods: Transparent containers, sports equipment, and appliance components.
  • Industrial hardware: Protective shields, gears, and structural supports.
makrolon 2207 pc resin application

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.