Plastic Granules
Makrolon 2407 RE25 CQ Polycarbonate Granules
Makrolon® 2407 RE25 CQ is a UV-stable, transparent polycarbonate resin with CQ renewable content (via ISCC PLUS mass balance). This low-viscosity, easy-release grade excels in injection molding for durable, eco-conscious components requiring clarity and weatherability.
Associated Documents
ISO TDS
Typical property data
Physical Properties (Rheological)
- Melt Volume-Flow Rate (300 °C/1.2 kg): 19 cm³/10 min (ISO 1133)
- Melt Mass-Flow Rate (300 °C/1.2 kg): 20 g/10 min (ISO 1133)
- Molding Shrinkage (Parallel): 0.65 % (ISO 294-4)
- Molding Shrinkage (Normal): 0.7 % (ISO 294-4)
Mechanical Properties (23 °C/50 % r. h.)
- Tensile Modulus: 2400 MPa (ISO 527-1,-2)
- Yield Stress: 66 MPa (ISO 527-1,-2)
- Yield Strain: 6.0 % (ISO 527-1,-2)
- Nominal Strain at Break: > 50 % (ISO 527-1,-2)
- Flexural Modulus: 2350 MPa (ISO 178)
- Flexural Strength: 98 MPa (ISO 178)
- Charpy Notched Impact Strength (23 °C/3 mm): 65 kJ/m² (ISO 21305)
- Charpy Notched Impact Strength (-30 °C/3 mm): 14 kJ/m² (ISO 21305)
- Puncture Impact (Maximum Force at 23 °C): 5100 N (ISO 6603-2)
- Ball Indentation Hardness: 116 N/mm² (ISO 2039-1)
Thermal Properties
- Glass Transition Temperature: 143 °C (ISO 11357-1,-2)
- Temperature of Deflection Under Load (1.80 MPa): 124 °C (ISO 75-1,-2)
- Temperature of Deflection Under Load (0.45 MPa): 136 °C (ISO 75-1,-2)
- Vicat Softening Temperature (50 N, 50 °C/h): 143 °C (ISO 306)
- Thermal Conductivity (23 °C): 0.20 W/(m·K) (ISO 8302)
- Coefficient of Linear Thermal Expansion: 0.65 × 10⁻⁴/K (ISO 11359-1,-2)
- Oxygen Index: 27 % (ISO 4589-2)
Electrical Properties (23 °C/50 % r. h.)
- Relative Permittivity (100 Hz): 3.1 (IEC 60250)
- Dissipation Factor (100 Hz): 5 × 10⁻⁴ (IEC 60250)
- Volume Resistivity: 1E14 Ohm·m (IEC 62631-3-1)
- Surface Resistivity: 1E16 Ohm (IEC 62631-3-2)
- Electrical Strength (1 mm): 34 kV/mm (IEC 60243-1)
- Comparative Tracking Index (CTI, Solution A): 250 (IEC 60112)
Other Properties (23 °C)
- Density: 1200 kg/m³ (ISO 1183-1)
- Water Absorption (Saturation Value): 0.30 % (ISO 62)
- Water Absorption (Equilibrium Value, 23 °C, 50 % r. h.): 0.12 % (ISO 62)
- Refractive Index: 1.584 (ISO 489)
- Luminous Transmittance (Clear, 2 mm): 89 % (ISO 13468-2)
Processing and Drying Conditions
- Melt Temperature: 280 – 320 °C (Standard: 300 °C)
- Mold Temperature: 80 – 120 °C
- Drying Temperature: 120 °C
- Drying Time: 2 – 3 h
- Moisture Content (max): ≤ 0.02 %
- Injection Velocity: 200 mm/s (ISO 294)
Features & Benefits
Sustainable Material Choice
Partially bio-circular (attributed via mass balance), it reduces carbon footprint without sacrificing performance. Ideal for brands prioritizing eco-compliance and lifecycle transparency.
Superior UV Resistance
Built-in UV stabilization prevents yellowing and degradation in outdoor use. Ensures long-term clarity for applications like lighting covers or automotive trims exposed to sunlight.
Easy Processing & Release
Low viscosity (19 cm³/10 min MVR) and mold-release properties cut cycle times and reduce defects. Lowers production costs for complex geometries like thin-walled housings.
Use & Applications
- Outdoor Lighting: LED diffusers, streetlight covers (UV-resistant clarity).
- Consumer Electronics: Transparent device housings (scratch/impact-resistant).
- Automotive Glazing: Interior lenses, sunroof components (thermal stability).
- Industrial Shields: Safety visors, machine guards (high optical transmission).