Covestro Makrolon® 6485 PC Resin

Makrolon 6485 PC Resin Flame Retardant

Covestro Makrolon® 6485 is a flame-retardant, medium-viscosity polycarbonate resin engineered for demanding industrial applications. With UL 94 V-0 (1.5 mm) and 5VA (3.0 mm) certifications, easy-release properties, and opaque color options, it ensures safety and efficiency in injection molding (280–320°C melt temps).

covestro makrolon® pc resin 25kg package

Download PDF

Typical property data

Physical Properties (Rheological)
  • Melt volume-flow rate (300 °C/1.2 kg): 9 cm³/10 min (ISO 1133)
  • Melt mass-flow rate (300 °C/1.2 kg): 10 g/10 min (ISO 1133)
  • Molding shrinkage, parallel (60x60x2 mm³/500 bar): 0.65% (ISO 294-4)
  • Molding shrinkage, normal (60x60x2 mm³/500 bar): 0.7% (ISO 294-4)
  • Molding shrinkage range (parallel/normal): 0.6−0.8% (ISO 2577)
Mechanical Properties (23 °C/50 % r. h.)
  • Tensile modulus (1 mm/min): 2400 MPa (ISO 527-1,-2)
  • Yield stress (50 mm/min): 66 MPa (ISO 527-1,-2)
  • Yield strain (50 mm/min): 6.1% (ISO 527-1,-2)
  • Nominal strain at break (50 mm/min): >50% (ISO 527-1,-2)
  • Tensile creep modulus (1 h): 2200 MPa (ISO 899-1)
  • Tensile creep modulus (1000 h): 1900 MPa (ISO 899-1)
  • Flexural modulus (2 mm/min): 2400 MPa (ISO 178)
  • Flexural strength (2 mm/min): 98 MPa (ISO 178)
  • Charpy notched impact strength (23 °C/3 mm): 70 kJ/m² (ISO 21305/ISO 179/1eA)
  • Charpy notched impact strength (-30 °C/3 mm): 14 kJ/m² (ISO 21305/ISO 179/1eA)
Thermal Properties
  • Glass transition temperature (10 °C/min): 142 °C (ISO 11357-1,-2)
  • Temperature of deflection under load (1.80 MPa): 124 °C (ISO 75-1,-2)
  • Vicat softening temperature (50 N, 50 °C/h): 144 °C (ISO 306)
  • Burning behavior (1.5 mm): UL 94 V-0
  • Burning behavior (3.0 mm): UL 94 5VA
  • Oxygen index: 36% (ISO 4589-2)
Electrical Properties (23 °C/50 % r. h.)
  • Relative permittivity (100 Hz): 3.1 (IEC 60250)
  • Relative permittivity (1 MHz): 3.0 (IEC 60250)
  • Electrical strength (1 mm): 34 kV/mm (IEC 60243-1)
Other Properties (23 °C)
  • Water absorption (saturation value, 23 °C): 0.30% (ISO 62)
  • Water absorption (equilibrium value, 50 % r. h.): 0.12% (ISO 62)
  • Density: 1200 kg/m³ (ISO 1183-1)
Processing and Drying Conditions
  • Melt temperature (injection molding): 280−320 °C
  • Mold temperature (injection molding): 80−120 °C
  • Drying temperature (dry air): 120 °C
  • Drying time (dry air): 2−3 h
  • Moisture content (max): ≤0.02%

Use & Applications

  • Electrical Enclosures: Flame-retardant housings for switches, circuit breakers, and power distribution units.
  • Automotive Components: Sensor casings, connectors, and under-hood parts requiring heat/impact resistance.
  • Consumer Electronics: Charger bodies, power tool housings, and appliance guards.
  • Industrial Safety: Control panels, machinery covers, and fire-rated equipment parts.
covestro makrolon 6485 application
covestro makrolon 6485 application

Features & Benefits

Reliable Flame Resistance

Makrolon 6485 delivers UL 94 V-0/5VA ratings, critical for electronics and automotive parts exposed to high heat or electrical risks, ensuring compliance without secondary treatments.

Optimized Processing Efficiency

Medium viscosity (9.0 cm³/10 min MVR) and easy-release properties reduce cycle times and mold fouling, cutting production costs for complex components like connectors or housings.

Tough Mechanical Performance

High impact strength (>50% nominal strain) and dimensional stability (0.6–0.8% shrinkage) guarantee durable parts that withstand drops, vibrations, and thermal shifts in harsh environments.

covestro makrolon® pc resin 25kg package

Makrolon® 6485 Related Flame Retardant Grades

Disclaimer: Grades below are potential alternatives for comparison only. Not direct drop-in replacements. Typical values from Covestro ISO TDS; verify UL94 colors/thickness on current UL Yellow Card. RoHS/REACH/halogen/PFAS status not confirmed unless report provided.

GradePositioningUL94 (ISO TDS)MVRHDT (1.80 MPa)Notched Impact (23°C/3mm)ColorUV / UL 746C f1
6487Medium viscosity; 5VA; UVV-0 @1.5mm; 5VA @3.0mm9.0 cm³/10min122°CCharpy 70P(C); Izod 70P(C)OpaqueYes / N/A
6487 REBio-circular (ISCC PLUS); 5VA; UVV-0 @1.5mm; 5VA @3.0mm9.0 cm³/10min122°CCharpy 70P(C); Izod 70P(C)OpaqueYes / N/A
941510% GF; 5VA; high viscosityV-0 @1.5mm; 5VA @3.0mm6.0 cm³/10min136°CCharpy 10C; Izod 10COpaqueNo / N/A
6265 XLow viscosity; opaqueV-0 @1.5mm19 cm³/10min124°CCharpy 65P(C); Izod 50P(C)OpaqueNo / N/A

👉 Full Portfolio: Browse all 27+ grades on the Covestro Flame Retardant PC Resin Hub.

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.