Covestro Makrolon® 6717 PC Resin

Makrolon 6717 PC Resin Flame Retardant Grades

Makrolon® 6717 is a flame-retardant, UV-stabilized polycarbonate resin with high viscosity and easy-release properties. It delivers UL 94 V-0 compliance at 2.0 mm thickness, excellent flow (MVR 3.0 cm³/10 min), and is available in transparent, translucent, and opaque colors for versatile design.

covestro makrolon® pc resin 25kg package

Download PDF

Typical Property Data

Physical Properties (Rheological)
  • Melt Volume-Flow Rate (MVR): 3.0 cm³/10 min (300 °C/1.2 kg, ISO 1133)
  • Melt Mass-Flow Rate (MFR): 3.0 g/10 min (300 °C/1.2 kg, ISO 1133)
  • Molding Shrinkage (Parallel): 0.7 % (60 × 60 × 2 mm³/500 bar, ISO 294-4)
  • Molding Shrinkage (Normal): 0.75 % (60 × 60 × 2 mm³/500 bar, ISO 294-4)
Mechanical Properties (23 °C/50 % r. h.)
  • Tensile Modulus: 2400 MPa (1 mm/min, ISO 527-1,-2)
  • Yield Stress: 67 MPa (50 mm/min, ISO 527-1,-2)
  • Yield Strain: 6.4 % (50 mm/min, ISO 527-1,-2)
  • Nominal Strain at Break: >50 % (50 mm/min, ISO 527-1,-2)
  • Flexural Modulus: 2400 MPa (2 mm/min, ISO 178)
  • Flexural Strength: 98 MPa (2 mm/min, ISO 178)
  • Charpy Notched Impact Strength (23 °C): 70 kJ/m² (3 mm, ISO 21305 based on ISO 179/1eA)
Thermal Properties
  • Glass Transition Temperature (Tg): 146 °C (10 °C/min, ISO 11357-1,-2)
  • Deflection Temperature Under Load (1.80 MPa): 127 °C (ISO 75-1,-2)
  • Deflection Temperature Under Load (0.45 MPa): 139 °C (ISO 75-1,-2)
  • Vicat Softening Temperature: 146 °C (50 N, 50 °C/h, ISO 306)
  • Burning Behavior: UL 94 V-0 (2.0 mm, UL 94)
Electrical Properties (23 °C/50 % r. h.)
  • Relative Permittivity (100 Hz): 3.1 (IEC 60250)
  • Relative Permittivity (1 MHz): 3.0 (IEC 60250)
  • Volume Resistivity: 1E14 Ohm·m (IEC 62631-3-1)
  • Surface Resistivity: 1E16 Ohm (IEC 62631-3-2)
  • Electrical Strength: 34 kV/mm (1 mm, IEC 60243-1)
Other Properties (23 °C)
  • Density: 1200 kg/m³ (ISO 1183-1)
  • Water Absorption (Equilibrium): 0.12 % (23 °C, 50 % r. h., ISO 62)
Processing and Drying Conditions
  • Melt Temperature: 280–320 °C (Recommended)
  • Injection Mold Temperature: 80–120 °C
  • Drying Temperature: 120 °C
  • Drying Time: 2–3 hours
  • Moisture Content (Max.): ≤0.02 %

Use & Applications

  • Electrical: Circuit breakers, EV battery covers
  • Transportation: Aircraft interior panels (FAR 25.853 compliant), train components
  • Industrial: Flame-retardant housings for power tools/machinery
  • Consumer: Safety visors, smart device casings
  • Lighting: LED diffusers (87% light transmittance @ 1mm)
covestro makrolon® pc resin 25kg package

Features & Benefits

Safety-Built Material

Makrolon 6717 achieves UL 94 V-0 flame retardancy at just 2.0 mm thickness, ideal for electrical enclosures or EV components where fire safety is critical.

Unmatched Toughness

With >105% strain at break (ISO 527) and high puncture resistance (65 J at -30°C), it withstands impacts in demanding environments like medical devices or industrial tools.

Processing Flexibility

Branched chain structure ensures smooth flow at 280–320°C melt temps, enabling complex thin-wall molding and reducing cycle times for high-volume production.

covestro makrolon® pc resin 25kg package

Makrolon® 6717 Related Flame Retardant Grades

Disclaimer: Grades below are potential alternatives for comparison only. Not direct drop-in replacements. Typical values from Covestro ISO TDS; verify UL94 colors/thickness on current UL Yellow Card. RoHS/REACH/halogen/PFAS status not confirmed unless report provided.

GradePositioningUL94 (ISO TDS)MVRHDT (1.80 MPa)Notched Impact (23°C/3mm)ColorUV / UL 746C f1
1804Extrusion; high viscosity; UV; sheetV-2 @1.5mm; V-0 @6.0mm6.0 cm³/10min127°CCharpy 80P; Izod 70PT/T/OYes / N/A
6557Medium viscosity; UV; transparentV-2 @1.5mm; V-0 @3.0mm10 cm³/10min124°CCharpy 70P(C); Izod 65PT/T/OYes / N/A
6457Medium viscosity; UV; transparentV-2 @1.5mm; V-0 @3.0mm12 cm³/10min123°CCharpy 70P(C); Izod 65PT/OYes / N/A
FR7087Medium viscosity; UV; E/EV-2 @1.5mm; V-0 @2.2mm; 5VA @3.0mm12 cm³/10min106°CIzod 8C; 8C @-30°CT/TYes / N/A

👉 Full Portfolio: Browse all 27+ grades on the Covestro Flame Retardant PC Resin Hub.

Send Us a Message