Covestro Makrolon® AL2647 RE CQ PC Resin

covestro makrolon® pc resin 25kg package

Makrolon AL2647 RE CQ Polycarbonate Granules

Makrolon® AL2647 RE CQ is a medium-viscosity, UV-stabilized polycarbonate resin featuring easy mold release and partial bio-circular content via ISCC PLUS mass balance. Ideal for injection molding, it delivers exceptional clarity in transparent/signal colors for demanding applications like automotive lighting.

Associated Documents

ISO TDS

Typical property data

Physical Properties (Rheological)
  • Melt Volume-Flow Rate (MVR): 12 cm³/10 min (300 °C/1.2 kg, ISO 1133)
  • Melt Mass-Flow Rate (MFR): 13 g/10 min (300 °C/1.2 kg, ISO 1133)
  • Molding Shrinkage (Parallel): 0.7% (60 × 60 × 2 mm³/500 bar, ISO 294-4)
  • Molding Shrinkage (Normal): 0.75% (60 × 60 × 2 mm³/500 bar, ISO 294-4)
Mechanical Properties (23 °C/50% r. h.)
  • Tensile Modulus: 2400 MPa (1 mm/min, ISO 527-1, -2)
  • Yield Stress: 67 MPa (50 mm/min, ISO 527-1, -2)
  • Yield Strain: 6.1% (50 mm/min, ISO 527-1, -2)
  • Nominal Strain at Break: > 50% (50 mm/min, ISO 527-1, -2)
  • Tensile Creep Modulus (1 h): 2200 MPa (ISO 899-1)
  • Tensile Creep Modulus (1000 h): 1900 MPa (ISO 899-1)
  • Flexural Modulus: 2400 MPa (2 mm/min, ISO 178)
  • Flexural Strength: 98 MPa (2 mm/min, ISO 178)
  • Charpy Notched Impact Strength (23 °C, 3 mm): 70 kJ/m² (ISO 21305/ISO 179/1eA)
  • Charpy Notched Impact Strength (-30 °C, 3 mm): 14 kJ/m² (ISO 21305/ISO 179/1eA)
  • Puncture Impact Maximum Force (23 °C): 5400 N (ISO 6603-2)
  • Puncture Energy (23 °C): 60 J (ISO 6603-2)
Thermal Properties
  • Glass Transition Temperature: 144 °C (10 °C/min, ISO 11357-1, -2)
  • Temperature of Deflection Under Load (1.80 MPa): 123 °C (ISO 75-1, -2)
  • Temperature of Deflection Under Load (0.45 MPa): 136 °C (ISO 75-1, -2)
  • Vicat Softening Temperature: 143 °C (50 N, 50 °C/h, ISO 306)
  • Coefficient of Linear Thermal Expansion (Parallel/Normal): 0.65 × 10⁻⁴/K (23–55 °C, ISO 11359-1, -2)
  • Burning Behavior (UL 94): V-2 (0.75 mm), HB (2.5 mm)
Electrical Properties (23 °C/50% r. h.)
  • Relative Permittivity (100 Hz): 3.1 (IEC 60250)
  • Relative Permittivity (1 MHz): 3.0 (IEC 60250)
  • Dissipation Factor (100 Hz): 0.0005 (IEC 60250)
  • Dissipation Factor (1 MHz): 0.0090 (IEC 60250)
  • Volume Resistivity: 1 × 10¹⁴ Ω·m (IEC 62631-3-1)
  • Surface Resistivity: 1 × 10¹⁶ Ω (IEC 62631-3-2)
  • Electrical Strength: 34 kV/mm (1 mm, IEC 60243-1)
  • Comparative Tracking Index (CTI): 250 (IEC 60112)
Other Properties (23 °C)
  • Density: 1200 kg/m³ (ISO 1183-1)
  • Water Absorption (Saturation Value): 0.30% (23 °C, ISO 62)
  • Water Absorption (Equilibrium Value): 0.12% (23 °C, 50% r. h., ISO 62)
Processing and Drying Conditions
  • Injection Molding Melt Temperature: 280–320 °C (ISO 294)
  • Mold Temperature: 80–120 °C (ISO 294)
  • Drying Temperature: 120 °C (Dry Air)
  • Drying Time: 2–3 hours
  • Moisture Content (Max.): ≤ 0.02%

Features & Benefits

Sustainable Performance

This ISCC PLUS-certified resin uses bio-circular raw materials, reducing carbon footprint without compromising quality—perfect for eco-conscious automotive supply chains.

Optical Precision & Durability

With >87% light transmittance (4mm) and UV stabilization, it withstands weathering and maintains clarity for high-stress components like headlamp lenses.

Optimized Processing

Wide melt temperature range (280–320°C), low shrinkage (0.6–0.8%), and easy-release properties boost production efficiency and part consistency.

covestro makrolon® pc resin 25kg package

Use & Applications

  • Headlamp lenses (forward lighting systems)
  • Signal lights (e.g., indicators, brake lights)
  • Exterior light housings requiring UV/weather resistance