Plastic Granules
Makrolon AL2647 RP70 CQ Polycarbonate Granules
Makrolon AL2647 RP70 CQ is a UV-stabilized, partially circular polycarbonate resin made from post-consumer recycled content via ISCC PLUS mass balance. Designed for automotive lighting, it offers exceptional optical clarity, easy release, and injection molding versatility in transparent/signal colors.
Download PDF
ISO TDS
Typical property data
Physical Properties (Rheological)
- Melt Volume-Flow Rate (MVR): 12 cm³/10 min (ISO 1133, at 300 °C/1.2 kg)
- Melt Mass-Flow Rate (MFR): 13 g/10 min (ISO 1133, at 300 °C/1.2 kg)
- Molding Shrinkage (Parallel): 0.7 % (ISO 294-4, at 60x60x2 mm³/500 bar)
- Molding Shrinkage (Normal): 0.75 % (ISO 294-4, at 60x60x2 mm³/500 bar)
Mechanical Properties (23 °C/50 % r. h.)
- Tensile Modulus: 2400 MPa (ISO 527-1,-2, at 1 mm/min)
- Yield Stress: 67 MPa (ISO 527-1,-2, at 50 mm/min)
- Yield Strain: 6.1 % (ISO 527-1,-2, at 50 mm/min)
- Nominal Strain at Break: >50 % (ISO 527-1,-2, at 50 mm/min)
- Flexural Modulus: 2400 MPa (ISO 178, at 2 mm/min)
- Flexural Strength: 98 MPa (ISO 178, at 2 mm/min)
- Charpy Notched Impact Strength (23 °C, 3 mm): 70 kJ/m² (ISO 21305/ISO 179/1eA)
- Charpy Notched Impact Strength (-30 °C, 3 mm): 14 kJ/m² (ISO 21305/ISO 179/1eA)
Thermal Properties
- Glass Transition Temperature: 144 °C (ISO 11357-1,-2)
- Deflection Temperature Under Load (1.80 MPa): 123 °C (ISO 75-1,-2)
- Deflection Temperature Under Load (0.45 MPa): 136 °C (ISO 75-1,-2)
- Vicat Softening Temperature (50 N, 50 °C/h): 143 °C (ISO 306)
- Oxygen Index: 28 % (ISO 4589-2)
Electrical Properties (23 °C/50 % r. h.)
- Relative Permittivity (100 Hz): 3.1 (IEC 60250)
- Relative Permittivity (1 MHz): 3.0 (IEC 60250)
- Electrical Strength: 34 kV/mm (1 mm, IEC 60243-1)
Other Properties (23 °C)
- Density: 1200 kg/m³ (ISO 1183-1)
- Water Absorption (Saturation): 0.30 % (ISO 62, Water at 23 °C)
- Water Absorption (Equilibrium): 0.12 % (ISO 62, at 23 °C/50 % r. h.)
Processing and Drying Conditions
- Melt Temperature (Injection Molding): 280−320 °C
- Standard Melt Temperature: 300 °C (ISO 294)
- Mold Temperature (Injection Molding): 80−120 °C (ISO 294)
- Drying Temperature: 120 °C
- Drying Time: 2−3 h
Use & Applications
- Headlamp lenses (forward lighting)
- Signal lighting housings (e.g., brake lights, indicators)
- Durable transparent covers for sensors/electronics
- UV-exposed exterior parts requiring color stability
Features & Benefits
Eco-Certified Recycled Content
This ISCC PLUS-attributed resin uses chemically recycled post-consumer materials, reducing environmental impact while meeting stringent automotive sustainability goals.
Superior Optical Performance
With 89% light transmittance (1mm) and <0.5% haze, it ensures crystal-clear lenses for headlamps, maintaining UV stability under harsh outdoor conditions.
Reliable Processing & Durability
Medium viscosity enables smooth injection molding (280–320°C), while high impact strength (70 kJ/m²) and 123°C heat deflection prevent warping/cracking in demanding applications.