Covestro Makrolon® AX2675 RE PC Resin

covestro makrolon® pc resin 25kg package

Makrolon AX2675 RE Polycarbonate Granules Black color

Makrolon® AX2675 RE by Covestro is a medium-viscosity, easy-release polycarbonate resin with an MVR of 12 cm³/10 min (300°C/1.2 kg). Designed for high-gloss automotive exteriors, it offers partial bio-circular sustainability (ISCC PLUS mass balance) and is exclusively available in black.

Associated Documents

ISO TDS

Typical property data

Physical Properties (Rheological)
  • Melt Volume-Flow Rate (300 °C/1.2 kg): 12 cm³/10 min (ISO 1133)
  • Melt Mass-Flow Rate (300 °C/1.2 kg): 13 g/10 min (ISO 1133)
  • Molding Shrinkage (Parallel, 60x60x2 mm³/500 bar): 0.7% (ISO 294-4)
  • Molding Shrinkage (Normal, 60x60x2 mm³/500 bar): 0.75% (ISO 294-4)
  • Molding Shrinkage Range (Parallel/Normal): 0.6–0.8% (ISO 2577)
Mechanical Properties (23 °C/50 % r.h.)
  • Tensile Modulus (1 mm/min): 2400 MPa (ISO 527-1,-2)
  • Yield Stress (50 mm/min): 65 MPa (ISO 527-1,-2)
  • Yield Strain (50 mm/min): 6.0% (ISO 527-1,-2)
  • Nominal Strain at Break (50 mm/min): >50% (ISO 527-1,-2)
  • Flexural Modulus (2 mm/min): 2400 MPa (ISO 178)
  • Flexural Strength (2 mm/min): 98 MPa (ISO 178)
  • Charpy Notched Impact Strength (23 °C, 3 mm): 70 kJ/m² (ISO 21305/ISO 179/1eA)
  • Charpy Notched Impact Strength (-30 °C, 3 mm): 16 kJ/m² (ISO 21305/ISO 179/1eA)
  • Puncture Impact Maximum Force (23 °C): 5200 N (ISO 6603-2)
  • Puncture Impact Maximum Force (-30 °C): 6100 N (ISO 6603-2)
Thermal Properties
  • Glass Transition Temperature (10 °C/min): 143 °C (ISO 11357-1,-2)
  • Temperature of Deflection Under Load (1.80 MPa): 124 °C (ISO 75-1,-2)
  • Temperature of Deflection Under Load (0.45 MPa): 136 °C (ISO 75-1,-2)
  • Vicat Softening Temperature (50 N, 50 °C/h): 143 °C (ISO 306)
  • Thermal Conductivity (23 °C, through-plane): 0.20 W/(m·K) (ISO 8302)
  • Coefficient of Linear Thermal Expansion (23–55 °C, Parallel/Normal): 0.65 × 10⁻⁴/K (ISO 11359-1,-2)
Electrical Properties (23 °C/50 % r.h.)
  • Relative Permittivity (100 Hz): 3.1 (IEC 60250)
  • Relative Permittivity (1 MHz): 3.0 (IEC 60250)
  • Dissipation Factor (100 Hz): 0.0005 (IEC 60250)
  • Dissipation Factor (1 MHz): 0.009 (IEC 60250)
  • Volume Resistivity: 1 × 10¹⁴ Ω·m (IEC 62631-3-1)
  • Surface Resistivity: 1 × 10¹⁶ Ω (IEC 62631-3-2)
  • Electrical Strength (1 mm): 34 kV/mm (IEC 60243-1)
  • Comparative Tracking Index (Solution A): 250 (IEC 60112)
Other Properties (23 °C)
  • Density: 1200 kg/m³ (ISO 1183-1)
  • Water Absorption (Saturation): 0.30% (ISO 62)
  • Water Absorption (Equilibrium, 50% RH): 0.12% (ISO 62)
Processing and Drying Conditions
  • Injection Molding Melt Temperature: 280–320 °C (ISO 294)
  • Mold Temperature: 80–120 °C (ISO 294)
  • Drying Temperature: 120 °C
  • Drying Time: 2–3 hours
  • Moisture Content (Max): ≤0.02%
  • Injection Velocity: 200 mm/s (ISO 294)

Features & Benefits

Sustainable Material Choice

This Covestro Makrolon® AX2675 RE uses bio-circular attribution (ISCC PLUS), reducing carbon footprint while meeting automotive standards—ideal for eco-driven procurement.

Premium Surface Performance

Engineered for flawless high-gloss finishes, it resists scratches and maintains aesthetics under harsh conditions, perfect for luxury automotive trims.

Effortless Processing

Medium viscosity and easy-release properties enable faster injection molding cycles, cutting production costs without sacrificing part precision.

covestro makrolon® pc resin 25kg package

Use & Applications

  • Automotive Exterior Trims: Roof strips and pillar appliqués demanding UV resistance and high-gloss finishes.
  • Premium Surfaces: High-gloss components for luxury vehicles, paired with hard coatings for scratch protection.
  • Injection-Molded Parts: Complex geometries requiring dimensional stability (e.g., sensor housings).
  • Sustainable Solutions: Eco-conscious automotive projects leveraging bio-circular materials.
makrolon ax2675 re pc resin application

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.