Makrolon ET3113 PC Resin High-viscosity UV-stabilized
Covestro Makrolon ET3113 is a high-viscosity, UV-stabilized polycarbonate resin designed for extrusion applications. With an MVR of 6.0 cm³/10 min (300°C/1.2kg), it delivers exceptional impact resistance and optical clarity, exclusively in transparent colors for demanding industrial use.
Associated Documents
ISO TDS
Typical property data
Physical Properties (Rheological)
- Melt Volume-Flow Rate: 6.0 cm³/10 min (300 °C/1.2 kg) (ISO 1133)
- Melt Mass-Flow Rate: 6.5 g/10 min (300 °C/1.2 kg) (ISO 1133)
- Molding Shrinkage (Parallel): 0.7 % (60x60x2 mm³/500 bar) (ISO 294-4)
- Molding Shrinkage (Normal): 0.75 % (60x60x2 mm³/500 bar) (ISO 294-4)
Mechanical Properties (23 °C/50 % r. h.)
- Tensile Modulus: 2350 MPa (1 mm/min) (ISO 527-1,-2)
- Yield Stress: 65 MPa (50 mm/min) (ISO 527-1,-2)
- Yield Strain: 6.3 % (50 mm/min) (ISO 527-1,-2)
- Nominal Strain at Break: >50 % (50 mm/min) (ISO 527-1,-2)
- Flexural Modulus: 2350 MPa (2 mm/min) (ISO 178)
- Flexural Strength: 96 MPa (2 mm/min) (ISO 178)
- Charpy Notched Impact Strength (23 °C/3 mm): 80 kJ/m² (ISO 21305/ISO 179/1eA)
- Izod Notched Impact Strength (23 °C/3 mm): 70 kJ/m² (ISO 21305/ISO 180/A)
- Puncture Impact Properties (Max Force): 5600 N (23 °C) (ISO 6603-2)
Thermal Properties
- Glass Transition Temperature: 148 °C (10 °C/min) (ISO 11357-1,-2)
- Deflection Temperature Under Load (1.8 MPa): 128 °C (ISO 75-1,-2)
- Deflection Temperature Under Load (0.45 MPa): 141 °C (ISO 75-1,-2)
- Vicat Softening Temperature: 148 °C (50 N; 50 °C/h) (ISO 306)
- Burning Behavior (UL 94):
- 1.5 mm: HB (UL 94)
- 0.75 mm: V-2 (UL 94)
- Oxygen Index: 28 % (ISO 4589-2)
- Relative Temperature Index (Electrical Strength): 125 °C (1.5 mm) (UL 746B)
Electrical Properties (23 °C/50 % r. h.)
- Relative Permittivity:
- 3.1 (100 Hz) (IEC 60250)
- 3.0 (1 MHz) (IEC 60250)
Other Properties (23 °C)
- Water Absorption (Saturation Value): 0.30 % (Water at 23 °C) (ISO 62)
- Density: 1200 kg/m³ (ISO 1183-1)
- Refractive Index: 1.587 (ISO 489)
- Luminous Transmittance (Clear, 2 mm): 89 % (ISO 13468-2)
Processing and Drying Conditions
- Injection Molding – Melt Temperature: 300 °C (ISO 294)
- Injection Molding – Mold Temperature: 80 °C (ISO 294)
- Injection Molding – Injection Velocity: 200 mm/s (ISO 294)
Features & Benefits
Unmatched Impact Resistance
Makrolon ET3113 withstands heavy impacts (e.g., 60J puncture energy at 23°C), reducing part failure in high-stress environments like machinery guards or safety barriers.
Superior Optical Clarity & UV Stability
Boasting 88% light transmission (3mm thickness) and <0.8% haze, it maintains transparency and resists yellowing under sunlight—ideal for skylights or display panels.
High-Temperature Resilience
With a Vicat softening point of 148°C and HDT of 128°C (1.8 MPa), it performs reliably in hot settings like automotive components or outdoor structures.
Use & Applications
- Extrusion: Durable profiles for conveyor systems, protective edging, and architectural trim.
- Solid Sheet: Shatter-resistant windows for factories, safety visors, and transparent machine covers.
- Corrugated Sheet: Weather-resistant roofing for greenhouses, warehouses, and stadiums.