Covestro Makrolon® FR7087 PC Resin

Makrolon FR7087 PC Resin Flame Retardant

Makrolon® FR7087 is a medium-viscosity, flame-retardant PC resin from Covestro, optimized for injection molding. With UL 94 V-0 (2.2 mm) and 5VA (3.0 mm) ratings, UV stabilization, and easy-release properties, it’s ideal for electrical/electronic components. Available in transparent/translucent colors.

covestro makrolon® pc resin 25kg package

Download PDF

Typical property data

Physical Properties (Rheological)
  • Melt Volume-Flow Rate (300 °C/1.2 kg): 12 cm³/10 min (ISO 1133)
  • Melt Mass-Flow Rate (300 °C/1.2 kg): 12 g/10 min (ISO 1133)
Mechanical Properties (23 °C/50 % r.h.)
  • Tensile Modulus (1 mm/min): 2500 MPa (ISO 527-1, -2)
  • Yield Stress (50 mm/min): 75 MPa (ISO 527-1, -2)
  • Yield Strain (50 mm/min): 5.0 % (ISO 527-1, -2)
  • Stress at Break (50 mm/min): 75 MPa (ISO 527-1, -2)
  • Strain at Break (50 mm/min): 100 % (ISO 527-1, -2)
  • Charpy Impact Strength (23 °C): Non-break (ISO 179/1eU)
Thermal Properties
  • Temperature of Deflection Under Load (1.80 MPa): 106 °C (ISO 75-1, -2)
  • Temperature of Deflection Under Load (0.45 MPa): 118 °C (ISO 75-1, -2)
  • Vicat Softening Temperature (50 N; 50 °C/h): 123 °C (ISO 306)
  • Vicat Softening Temperature (50 N; 120 °C/h): 124 °C (ISO 306)
  • Burning Behavior UL 94 (1.5 mm): V-2 (UL 94)
  • Burning Behavior UL 94 (2.2 mm): V-0 (UL 94)
  • Burning Behavior UL 94-5V (3.0 mm): 5VA (UL 94)
  • Glow Wire Flammability Index (GWFI, 1.5 mm/2.2 mm/3.0 mm): 960 °C (IEC 60695-2-12)
  • Glow Wire Ignition Temperature (GWIT, 1.5 mm/2.2 mm/3.0 mm): 930-960 °C (IEC 60695-2-13)
  • Relative Temperature Index (Tensile Strength, 1.5 mm): 85 °C (UL 746B)
  • Relative Temperature Index (Electric Strength, 1.5 mm): 125 °C (UL 746B)
Other Properties (23 °C)
  • Haze (3 mm, Transparent Materials): 0.9 % (ISO 14782)
  • Luminous Transmittance (3 mm): 88 % (ISO 13468-2)
Processing and Drying Conditions
  • Injection Molding Melt Temperature: 280-320 °C, Standard: 300 °C (ISO 294)
  • Mold Temperature: 70-110 °C (ISO 294)
  • Dry Air Drying Temperature: 90 °C
  • Drying Time: 4 hours
  • Moisture Content (max.): ≤ 0.02 %
  • Hold Pressure (% of Injection Pressure): 50-75 %
  • Plastic Back Pressure: 100-200 bar
  • Peripheral Screw Speed: 0.05-0.2 m/s

Use & Applications

  • Safety-Critical Housings: EV chargers, power tools, circuit breakers (UL compliance).
  • Transparent Covers: LED diffusers, meter panels (clarity + flame resistance).
  • Connectors & Sockets: High-heat endurance in compact designs.
  • Industrial Enclosures: UV-stabilized for outdoor use.
covestro makrolon® pc resin 25kg package

Features & Benefits

Uncompromised Fire Safety

It meets strict UL 94 V-0 (2.2 mm) and 5VA (3.0 mm) flammability standards, ensuring compliance in high-risk electrical applications. No need for secondary flame-retardant treatments.

Effortless High-Temp Processing

Medium flow (MVR 12 cm³/10 min) simplifies injection molding at 280–320°C. UV stabilization and easy mold release reduce rejects. Faster cycles, lower costs.

Design Freedom & Durability

Transparent/translucent color options maintain aesthetics while resisting yellowing. High impact strength (8 kJ/m² at 23°C/-30°C) survives drops and vibrations. Beauty that lasts.

covestro makrolon® pc resin 25kg package

Makrolon® FR7087 Related Grades

Disclaimer: Grades below are potential alternatives for comparison only. Not direct drop-in replacements. Typical values from Covestro ISO TDS; verify UL94 colors/thickness on current UL Yellow Card. RoHS/REACH/halogen/PFAS status not confirmed unless report provided.

GradePositioningUL94 (ISO TDS)MVRHDT (1.80 MPa)Notched Impact (23°C/3mm)ColorUV / UL 746C f1
6457Medium viscosity; UV; transparentV-2 @1.5mm; V-0 @3.0mm12 cm³/10min123°CCharpy 70P(C); Izod 65PT/OYes / N/A
6557Medium viscosity; UV; transparentV-2 @1.5mm; V-0 @3.0mm10 cm³/10min124°CCharpy 70P(C); Izod 65PT/T/OYes / N/A
6487Medium viscosity; 5VA; UV; opaqueV-0 @1.5mm; 5VA @3.0mm9.0 cm³/10min122°CCharpy 70P(C); Izod 70P(C)OpaqueYes / N/A
6717High viscosity, branched; UVV-0 @2.0mm3.0 cm³/10min127°CCharpy 70P; Izod 60PT/T/OYes / N/A