Makrolon Rx2530 by Covestro is a medical-grade polycarbonate resin engineered for critical healthcare applications. With medium viscosity (MVR 15 cm³/10 min) and ISO 10993-1 biocompatibility, it delivers exceptional clarity, radiation sterilization resilience, and reliability for transparent medical components.

Associated Documents

ISO TDS

Typical property data

Physical Properties (Rheological)
  • Melt Volume-Flow Rate (MVR): 15 cm³/10 min (300 °C/1.2 kg; ISO 1133)
  • Melt Mass-Flow Rate (MFR): 15.5 g/10 min (300 °C/1.2 kg; ISO 1133)
  • Molding Shrinkage (Parallel): 0.6% (60x60x2 mm³/500 bar; ISO 294-4)
  • Molding Shrinkage (Normal): 0.65% (60x60x2 mm³/500 bar; ISO 294-4)
Mechanical Properties (23 °C/50 % r.h.)
  • Tensile Modulus: 2400 MPa (1 mm/min; ISO 527-1,-2)
  • Yield Stress: 67 MPa (50 mm/min; ISO 527-1,-2)
  • Yield Strain: 6.1% (50 mm/min; ISO 527-1,-2)
  • Nominal Strain at Break: > 50% (50 mm/min; ISO 527-1,-2)
  • Stress at Break: 75 MPa (50 mm/min; ISO 527-1,-2)
  • Flexural Modulus: 2400 MPa (2 mm/min; ISO 178)
  • Flexural Strength: 100 MPa (2 mm/min; ISO 178)
  • Charpy Notched Impact Strength:
    • 70 kJ/m² (23 °C/3 mm; ISO 21305/ISO 179/1eA)
    • 14 kJ/m² (-30 °C/3 mm; ISO 21305/ISO 179/1eA)
  • Izod Notched Impact Strength:
    • 65 kJ/m² (23 °C/3 mm; ISO 21305/ISO 180/A)
    • 12 kJ/m² (-30 °C/3 mm; ISO 21305/ISO 180/A)
  • Puncture Impact Properties:
    • Maximum Force: 5300 N (23 °C; ISO 6603-2)
    • Puncture Energy: 60 J (23 °C; ISO 6603-2)
Thermal Properties
  • Glass Transition Temperature: 142 °C (10 °C/min; ISO 11357-1,-2)
  • Temperature of Deflection Under Load:
    • 122 °C (1.80 MPa; ISO 75-1,-2)
    • 134 °C (0.45 MPa; ISO 75-1,-2)
  • Vicat Softening Temperature:
    • 141 °C (50 N; 50 °C/h; ISO 306)
  • Coefficient of Linear Thermal Expansion (Parallel/Normal): 0.65 x 10⁻⁴/K (23–55 °C; ISO 11359-1,-2)
  • Thermal Conductivity: 0.20 W/(m·K) (Through-plane, 23 °C; ISO 8302)
Electrical Properties (23 °C/50 % r.h.)
  • Volume Resistivity: 1E14 Ω·m (IEC 62631-3-1)
  • Surface Resistivity: 1E16 Ω (IEC 62631-3-2)
Other Properties (23 °C)
  • Water Absorption (Saturation Value): 0.30% (Water at 23 °C; ISO 62)
  • Water Absorption (Equilibrium Value): 0.12% (23 °C; 50 % r.h.; ISO 62)
  • Density: 1200 kg/m³ (ISO 1183-1)
Processing and Drying Conditions
  • Melt Temperature: 280–320 °C (Recommended: 300 °C)
  • Mold Temperature: 80–120 °C
  • Drying Conditions:
    • Temperature: 120 °C
    • Time: 2–3 h
    • Max Moisture Content: ≤ 0.02%

Features & Benefits

Biocompatible & Safe for Medical Use

Covestro PC Makrolon Rx2530 meets rigorous ISO 10993-1 standards, ensuring safety in implants or devices. This minimizes regulatory risks while protecting patient health.

Withstands Radiation Sterilization

It maintains structural integrity after gamma/e-beam sterilization—ideal for reusable surgical tools or single-use devices. No yellowing or brittleness, even under high-energy exposure.

Superior Impact Resistance & Clarity

It boasts 70 kJ/m² notched impact strength (23°C) and optical transparency. Perfect for drop-resistant housings or clear fluid-viewing parts in ER equipment.

covestro makrolon® pc resin 25kg package

Use & Applications

  • Medical Devices: Surgical instrument housings, dialysis components.
  • Transparent Medical Parts: IV connectors, blood reservoirs, diagnostic cartridges.
  • Injection-Molded Sterilizable Items: Autoclavable trays, implant packaging.
covestro makrolon® pc resin 25kg package