Plastic Granules
CYCOLAC™ Resin FR15U Flame retardant ABS
Cycolac™ Resin FR15U is a flame-retardant ABS resin with UL94 V-0 and 5VA ratings. It offers excellent indoor UV resistance, good moldability, and elevated UL RTI performance. Ideal for electrical housings and molded parts requiring reliable flame protection.
Typical property data
Physical Properties
- Specific Gravity: 1.19 (ASTM D792)
- Density: 1.19 g/cm³ (ISO 1183)
- Mold Shrinkage, Flow, 3.2 mm: 0.5–0.7 % (SABIC Method)
- Melt Flow Rate, 230°C / 3.8 kg: 3.3 g/10 min (ASTM D1238)
- Melt Flow Rate, 220°C / 5.0 kg: 7 g/10 min (ISO 1133)
- Melt Volume Rate, MVR at 220°C / 10.0 kg: 40 cm³/10 min (ISO 1133)
- Melt Viscosity, 200°C, 1000 sec⁻¹: 3200 Poise (ASTM D3825)
Mechanical Properties
- Tensile Stress at Yield, Type I, 5 mm/min: 37 MPa (ASTM D638)
- Tensile Stress at Break, Type I, 5 mm/min: 30 MPa (ASTM D638)
- Tensile Strain at Yield, Type I, 5 mm/min: 2.4 % (ASTM D638)
- Tensile Strain at Break, Type I, 5 mm/min: 17 % (ASTM D638)
- Tensile Modulus, 5 mm/min: 2060 MPa (ASTM D638)
- Flexural Stress at Yield, 1.3 mm/min, 50 mm Span: 67 MPa (ASTM D790)
- Flexural Modulus, 1.3 mm/min, 50 mm Span: 2340 MPa (ASTM D790)
- Tensile Stress at Yield, 50 mm/min: 41 MPa (ISO 527)
- Tensile Strain at Break, 50 mm/min: 22.0 % (ISO 527)
- Tensile Modulus, 1 mm/min: 2210 MPa (ISO 527)
- Flexural Stress at Yield, 2 mm/min: 63 MPa (ISO 178)
- Flexural Modulus, 2 mm/min: 2260 MPa (ISO 178)
Impact Properties
- Izod Impact, Notched, 23°C: 213 J/m (ASTM D256)
- Instrumented Dart Impact Total Energy, 23°C: 28 J (ASTM D3763)
- Izod Impact, Notched, 80 × 10 × 4 mm, +23°C: 12 kJ/m² (ISO 180/1A)
Thermal Properties
- Vicat Softening Temperature, Rate B/50: 93°C (ASTM D1525)
- Vicat Softening Temperature, Rate B/50: 92°C (ISO 306)
- Heat Deflection Temperature, 0.45 MPa, 3.2 mm, Unannealed: 86°C (ASTM D648)
- Heat Deflection Temperature, 1.82 MPa, 3.2 mm, Unannealed: 75°C (ASTM D648)
- Coefficient of Thermal Expansion, -40°C to 40°C, Flow: 9.0E-05 1/°C (ASTM E831)
- Coefficient of Thermal Expansion, -40°C to 40°C, Cross Flow: 9.18E-05 1/°C (ASTM E831)
- Relative Temperature Index, Electrical: 90°C (UL 746B)
- Relative Temperature Index, Mechanical with Impact: 85°C (UL 746B)
- Relative Temperature Index, Mechanical without Impact: 90°C (UL 746B)
Electrical Properties
- Arc Resistance, Tungsten: PLC Code 7 (ASTM D495)
- Hot Wire Ignition: PLC Code 2 (UL 746A)
- High Voltage Arc Tracking Rate: PLC Code 4 (UL 746A)
- High Ampere Arc Ignition, Surface: PLC Code 4 (UL 746A)
- Comparative Tracking Index, UL: PLC Code 1 (UL 746A)
- Volume Resistivity: >1.0E+14 Ω·cm (IEC 60093)
- Dielectric Strength, in Oil, 3.2 mm: 20 kV/mm (IEC 60243-1)
Flammability
- UL Recognized 94V-0 Flame Class Rating: 1.49 mm (UL 94)
- UL Recognized 94-5VA Flame Class Rating: 2.79 mm (UL 94)
Processing Parameters
- Processing Method: Injection molding
- Drying Temperature: 80–90°C
- Drying Time: 2–4 hrs
- Drying Time, Cumulative: 8 hrs
- Maximum Moisture Content: 0.1 %
- Melt Temperature: 205–230°C
- Nozzle Temperature: 205–230°C
- Front / Zone 3 Temperature: 205–220°C
- Middle / Zone 2 Temperature: 200–210°C
- Rear / Zone 1 Temperature: 170–180°C
- Mold Temperature: 50–70°C
- Back Pressure: 0.3–0.7 MPa
- Screw Speed: 30–60 rpm
- Shot to Cylinder Size: 50–70 %
- Vent Depth: 0.038–0.051 mm
Use & Applications
- for electrical housings and molded parts requiring reliable flame protection.