Sabic CYCOLOY™ Resin CM8823 PC/ABS

sabic cycoloy pc abs resin 25kg package

Sabic Cycoloy CM8823 (PC/ABS) Resin

Cycoloy Resins CM8823 is a high-heat PC/ABS blend engineered for injection molding. It delivers an exceptional balance of strength, dimensional stability, and impact resistance for demanding applications.

Associated Documents

TDS Europe

Typical property data

Physical Properties
  • Density: 1.32 g/cm³ (ISO 1183)
  • Water Absorption (23°C, saturated): 0.2% (ISO 62-1)
  • Moisture Absorption (23°C, 50% RH): 0.05% (ISO 62)
  • Melt Volume Rate (MVR at 260°C/5.0 kg): 10 cm³/10 min (ISO 1133)
Mechanical Properties
  • Tensile Stress, yield (5 mm/min): 55 MPa (ISO 527)
  • Tensile Stress, break (5 mm/min): 45 MPa (ISO 527)
  • Tensile Strain, yield (5 mm/min): 3.3% (ISO 527)
  • Tensile Strain, break (5 mm/min): 10% (ISO 527)
  • Tensile Modulus (1 mm/min): 5000 MPa (ISO 527)
  • Flexural Stress, yield (2 mm/min): 100 MPa (ISO 178)
  • Flexural Modulus (2 mm/min): 4600 MPa (ISO 178)
Impact Properties
  • Izod Impact, notched (80104, +23°C): 6 kJ/m² (ISO 180/1A)
  • Izod Impact, notched (80104, -30°C): 5 kJ/m² (ISO 180/1A)
Thermal Properties
  • Coefficient of Thermal Expansion (CTE, -40°C to 40°C, flow): 3.9E-05 1/°C (ISO 11359-2)
  • Coefficient of Thermal Expansion (CTE, -40°C to 40°C, xflow): 5.7E-05 1/°C (ISO 11359-2)
  • Ball Pressure Test (125°C ± 2°C): PASSES (IEC 60695-10-2)
  • Vicat Softening Temperature (Rate B/120): 136°C (ISO 306)
  • Heat Deflection Temperature (HDT/Af, 1.8 MPa): 118°C (ISO 75/Af)
Injection Molding
  • Drying Temperature: 110 – 120°C
  • Drying Time: 2 – 6 hours
  • Maximum Moisture Content: 0.02%
  • Melt Temperature: 270 – 300°C
  • Nozzle Temperature: 260 – 290°C
  • Front (Zone 3) Temperature: 270 – 300°C
  • Middle (Zone 2) Temperature: 265 – 290°C
  • Rear (Zone 1) Temperature: 260 – 270°C
  • Mold Temperature: 60 – 100°C
  • Back Pressure: 0.3 – 0.7 MPa
  • Screw Speed: 40 – 70 rpm
  • Shot to Cylinder Size: 30 – 80%
  • Vent Depth: 0.038 – 0.076 mm

Features & Benefits

Withstands High-Temperature Environments

CYCOLOY CM8823 Resin maintains structural integrity with a Heat Deflection Temperature of 118°C, ensuring parts perform reliably in hot conditions without warping.

Excellent Strength and Stiffness

This material offers high modulus and flexural strength, providing the rigidity needed for large, thin-walled components that must resist bending or breaking under load.

Reliable Impact Resistance

With good notched Izod impact values even at -30°C, CYCOLOY Resin CM8823 helps prevent brittle fractures, ensuring product durability and longevity in tough conditions.

sabic cycoloy fr resins particles

Use & Applications

  • Automotive Interior & Exterior Parts:
  • Consumer Electronics Housings
  • Electrical Enclosures
sabic cycoloy pc abs resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.