Sabic CYCOLOY™ Resin CY8630 PC/ABS

sabic cycoloy pc abs resin 25kg package

Sabic Cycoloy CY8630 (PC/ABS) Resin

Cycoloy CY8630 Resin is a high-performance PC/ABS blend engineered for demanding automotive applications, offering an exceptional balance of impact strength, heat resistance, and processability.

Associated Documents

TDS Asia

Typical property data

Physical Properties
  • Specific Gravity: 1.15 (ASTM D792)
  • Density: 1.15 g/cm³ (ISO 1183)
  • Mold Shrinkage: 0.5%–0.7% (flow and cross-flow; SABIC method)
  • Water Absorption (23°C/24hrs): 0.3% (ISO 62-1)
  • Water Absorption (23°C/saturated): 0.6% (ISO 62-1)
  • Moisture Absorption (23°C / 50% RH): 0.2% (ISO 62)
Mechanical Properties
  • Tensile Stress (yield): 58 MPa (ISO 527)
  • Tensile Stress (break): 55 MPa (ISO 527)
  • Tensile Strain (yield): 5.2% (ISO 527)
  • Tensile Strain (break): 75% (ISO 527)
  • Tensile Modulus: 2250 MPa (ISO 527)
  • Flexural Stress (yield): 85 MPa (ISO 178)
  • Flexural Modulus: 2300 MPa (ISO 178)
Impact Properties
  • Izod Impact, Notched (23°C): 50 kJ/m² (ISO 180/1A)
  • Izod Impact, Notched (-30°C): 25 kJ/m² (ISO 180/1A)
  • Izod Impact, Unnotched (23°C): No break (ISO 180/1U)
  • Izod Impact, Unnotched (-30°C): No break (ISO 180/1U)
  • Charpy Impact, V-notch (23°C): 50 kJ/m² (ISO 179/1eA)
  • Charpy Impact, V-notch (-30°C): 25 kJ/m² (ISO 179/1eA)
Thermal Properties
  • Vicat Softening Temperature (Rate B/120): 133°C (ISO 306)
  • Heat Deflection Temperature (0.45 MPa): 128°C (ASTM D648)
  • Heat Deflection Temperature (1.82 MPa): 110°C (ASTM D648)
  • CTE (Flow, -40°C to 40°C): 7×10−5 1/°C7 \times 10^{-5}\, \text{1/°C} (ASTM E831)
  • CTE (Cross-flow, -40°C to 40°C): 8×10−5 1/°C8 \times 10^{-5}\, \text{1/°C} (ASTM E831)
Electrical Properties
  • Volume Resistivity: (>1.E+16) (IEC 60093)
Flame Characteristics
  • Ball Pressure Test at 75°C ±2°C (PASSED) (IEC 60695-10-2)
  • Maximum Ball Pressure Test Temperature: 100°C (IEC 60695-10-2)
Injection Molding
  • Drying Temperature: 95–105°C
  • Drying Time: 2–4 hours
  • Maximum Moisture Content: 0.02%
  • Melt Temperature: 260–290°C
  • Nozzle Temperature: 240–280°C
  • Mold Temperature: 60–90°C

Features & Benefits

Superior Impact Resistance at Low Temperatures

With high notched Izod and Charpy impact values, even at -30°C, this material ensures components resist cracking and brittleness, crucial for interior trims that must endure daily use and extreme climates.

Excellent Heat Resistance and Stability

Featuring a Heat Deflection Temperature of 110°C at 1.82 MPa, parts made from CYCOLOY CY8630 Resin maintain their shape and integrity in hot environments, such as a car dashboard under the summer sun.

Optimized for Easy Molding

Its balanced flow and thermal properties allow for smooth, efficient injection molding with less warpage, reducing production defects and cycle times for high-volume automotive part manufacturing.

sabic cycoloy fr resins particles

Use & Applications

  • Automotive Interior Trims
  • Dashboard Components and Assemblies
  • Interior Brackets and Mounts
  • Console and Door Panel Elements
sabic cycoloy pc abs resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.