Sabic CYCOLOY™ Resin HC1104HF PC/ABS

sabic cycoloy pc abs resin 25kg package

Sabic Cycoloy HC1104HF (PC/ABS) Resin

Cycoloy HC1104HF is a high-heat PC/ABS blend engineered for superior impact resistance and excellent flow, making it ideal for demanding, high-performance applications.

Associated Documents

TDS Americas

Typical property data

Physical Properties
  • Melt Flow Rate: 17 g/10 min (ASTM D1238)
  • Melt Volume Rate (MVR): 18 cm³/10 min (ISO 1133)
Mechanical Properties
  • Tensile Stress (Yield): 52 MPa (ISO 527)
  • Tensile Stress (Break): 46 MPa (ISO 527)
  • Tensile Strain (Yield): 4.7% (ISO 527)
  • Tensile Strain (Break): 102% (ISO 527)
  • Tensile Modulus: 2180 MPa (ISO 527)
  • Flexural Stress (Yield): 81 MPa (ISO 178)
  • Flexural Modulus: 2140 MPa (ISO 178)
Impact Properties
  • Izod Impact (Notched, 23°C): 45 kJ/m² (ISO 180/1A)
  • Izod Impact (Notched, 0°C): 40 kJ/m² (ISO 180/1A)
  • Izod Impact (Notched, -30°C): 37 kJ/m² (ISO 180/1A)
  • Charpy Impact Strength (23°C, V-Notch): 56 kJ/m² (ISO 179/1eA)
Thermal Properties
  • Heat Deflection Temperature (HDT):
    • At 0.45 MPa: 128°C (ISO 75/Bf)
    • At 1.82 MPa: 103°C (ISO 75/Af)
  • Vicat Softening Temperature: 121°C (ISO 306)
Injection Molding
  • Drying Temperature: 100–110°C
  • Drying Time: 2–4 hours
  • Maximum Moisture Content: 0.02%
  • Melt Temperature: 260–290°C
  • Nozzle Temperature: 240–280°C
  • Mold Temperature: 60–90°C

Features & Benefits

Exceptional High-Heat Resistance

With a Heat Deflection Temperature of 106°C at 1.82 MPa, this CYCOLOY HC1104HF Resin withstands high-temperature environments, preventing deformation in applications like automotive interiors and electronics enclosures.

Superior Impact Strength & Durability

It offers excellent notched Izod impact resistance (583 J/m at 23°C), ensuring your products can endure rough handling and sudden impacts without cracking, which enhances product longevity and reduces failure rates.

Excellent Melt Flow for Processing

The high melt flow rate (17 g/10min) allows the HC1104HF to fill complex and thin-walled molds easily, resulting in faster cycle times and improved manufacturing efficiency for intricate part designs.

sabic cycoloy fr resins particles

Use & Applications

  • Automotive Interior Components (e.g., dashboard panels, trim, glove boxes)
  • Consumer Electronics Housings (e.g., laptops, power tool bodies, connectors)
  • Durable Thin-Walled Applications
  • Enclosures Requiring UL Recognition
  • Components Exposed to High Ambient Temperatures