Sabic CYCOLOY™ Resin MC1300 PC/ABS

sabic cycoloy pc abs resin 25kg package

Sabic Cycoloy MC1300 (PC/ABS) Resin

Cycoloy Resins MC1300 is a PC/ABS blend offering excellent flow and impact performance, ideal for plating and painting applications. It delivers the perfect balance of strength, processability, and superior surface finish.

Associated Documents

TDS Asia
TDS Americas

Typical property data

Physical Properties
  • Specific Gravity: 1.1 (ASTM D792)
  • Water Absorption (23°C/24 hrs): 0.1% (ASTM D570)
  • Mold Shrinkage (Flow, 3.2 mm): 0.5–0.8% (SABIC Method)
  • Mold Shrinkage (X-flow, 3.2 mm): 0.5–0.7% (SABIC Method)
  • Melt Flow Rate (260°C/5.0 kgf): 14 g/10 min (ASTM D1238)
Mechanical Properties
  • Tensile Stress (Yield, Type I, 50 mm/min): 50 MPa (ASTM D638)
  • Tensile Stress (Break, Type I, 50 mm/min): 44 MPa (ASTM D638)
  • Tensile Strain (Yield, Type I, 50 mm/min): 8.6% (ASTM D638)
  • Tensile Strain (Break, Type I, 50 mm/min): 150% (ASTM D638)
  • Tensile Modulus (50 mm/min): 2130 MPa (ASTM D638)
  • Flexural Stress (Yield, 1.3 mm/min, 50 mm span): 72 MPa (ASTM D790)
  • Flexural Modulus (1.3 mm/min, 50 mm span): 2100 MPa (ASTM D790)
Impact Properties
  • Izod Impact, Notched (23°C): 534 J/m (ASTM D256)
  • Izod Impact, Notched (-30°C): 427 J/m (ASTM D256)
  • Instrumented Dart Impact Total Energy (23°C): 41 J (ASTM D3763)
  • Instrumented Dart Impact Total Energy (-30°C): 33 J (ASTM D3763)
Thermal Properties
  • Vicat Softening Temperature (Rate B/50): 112°C (ASTM D1525)
  • Heat Deflection Temperature (HDT, 0.45 MPa, 3.2 mm, Unannealed): 115°C (ASTM D648)
  • Heat Deflection Temperature (HDT, 1.82 MPa, 3.2 mm, Unannealed): 99°C (ASTM D648)
  • Coefficient of Thermal Expansion (CTE, -40°C to 40°C, Flow): 7.2E-05, 1/°C (ASTM E831)
  • Coefficient of Thermal Expansion (CTE, -40°C to 40°C, X-flow): 9.E-05,1/°C (ASTM E831)
  • Thermal Conductivity: 0.2 W/m-°C (ASTM C177)
Injection Molding
  • Drying Temperature: 100–105°C
  • Drying Time: 3–4 hrs (Cumulative: 8 hrs)
  • Maximum Moisture Content: 0.02%
  • Melt Temperature: 260–290°C
  • Nozzle Temperature: 260–290°C
  • Mold Temperature: 75–100°C
  • Back Pressure: 0.3–0.7 MPa
  • Screw Speed: 40–70 rpm
  • Shot to Cylinder Size: 30–80%
  • Vent Depth: 0.038–0.076 mm

Features & Benefits

Superior Impact Strength & Toughness

With high Izod and Charpy impact values, even at low temperatures, CYCOLOY MC1300 ensures your components resist cracking and withstand sudden impacts during assembly and daily use.

Excellent Flow for Complex Molds

Its high melt flow rate allows CYCOLOY Resin MC1300 to easily fill thin walls and intricate mold geometries, reducing injection pressure and minimizing part defects like short shots or weld lines.

High Heat Resistance for Durable Parts

With a Heat Deflection Temperature (HDT) up to 115°C, components made from CYCOLOY MC1300 maintain their structural integrity in high-temperature environments, such as inside automotive interiors or near electronics.

sabic cycoloy fr resins particles

Use & Applications

  • Automotive Interior Trims (e.g., plated grilles, painted panels)
  • Consumer Electronics Housings (e.g., laptop bezels, tablet frames)
  • Durable Industrial Components and Housings
  • Household Appliances and Power Tool Casings