Eastech B432E General-purpose Extrusion Grade
Eastech B432E is a general-purpose extrusion-grade ABS resin known for its balanced rigidity, toughness, and superior thermal stability. Ideal for thin and thick sheet extrusion, this material supports a wide array of industrial applications with exceptional efficiency and quality.
Typical property data
Physical Properties
- Density: 1.04 g/cm³ (ISO 1183, 23°C)
- Melt Mass-Flow Rate (MFR): 5.5 g/10min (ISO 1133, 220°C/10kg)
- Molding Shrinkage: 0.4%−0.7% (ISO 294/4, 23°C)
Mechanical Properties
- Tensile Strength at Yield: 48 MPa (ISO 527, 50 mm/min)
- Tensile Elongation at Break: 15% (ISO 527, 50 mm/min)
- Tensile Modulus: 2300 MPa (ISO 527, 1 mm/min)
- Flexural Strength: 75 MPa (ISO 178, 2 mm/min)
- Flexural Modulus: 2300 MPa (ISO 178, 2 mm/min)
Impact Properties
- Izod Notched Impact Strength: 19 kJ/m² (ISO 180/1A, 23°C, 5.5J)
Thermal Properties
- Heat Deformation Temperature (HDT): 82 °C (ISO 75-2/A, 1.8 MPa)
- Vicat Softening Temperature: 102 °C (ISO 306, 50N, 50°C/h)
Process Guide
- Pre-drying Requirement: 2−4 hours @ 80°C (if no venting is available; air circulating oven)
- Melt Temperature: 190−230°C
Features & Benefits
Superior Thermal Stability
Eastech B432E offers excellent heat resistance, ensuring reliable performance for demanding extrusion and molding applications.
Exceptional Surface Smoothness
This resin delivers a high-quality finish, making it ideal for visible components in automobiles and furniture.
Balanced Rigidity and Toughness
The material’s perfect strength-flexibility balance makes it versatile for packaging, hygiene, and refrigeration industries.
Use & Applications
- Refrigeration: Durable panels for cooling systems.
- Hygiene Products: Smooth, resilient surfaces for bathroom interiors.
- Automobiles: Impact-resistant and finely finished trims.
- Packaging: Robust yet lightweight containers.