Eastech Chemical B532E ABS

shandong eastech abs resin 25kg package

Eastech B532E General-purpose Extrusion Grade

Eastech B532E is a general-purpose extrusion-grade ABS plastic resin designed for optimal performance in a variety of applications. With a balanced combination of rigidity, toughness, and excellent surface smoothness, it ensures reliability in industrial uses across multiple sectors.

Associated Documents

TDS - Data Sheet
ABS SVHC
ABS FDA
ABS ROHS
ABS TSCA
ABS POPs
ABS PAHs

Typical property data

Physical Properties
  • Density: 1.04 g/cm³ (ISO 1183, at 23°C)
  • Melt Mass-Flow Rate (MFR): 5.5 g/10 min (ISO 1133, 220°C/10 kg)
  • Molding Shrinkage: 0.4–0.7% (ISO 294/4, at 23°C)
Mechanical Properties
  • Tensile Strength at Yield: 48 MPa (ISO 527, 50 mm/min)
  • Tensile Elongation at Break: 15% (ISO 527, 50 mm/min)
  • Tensile Modulus: 2300 MPa (ISO 527, 1 mm/min)
  • Flexural Strength: 70 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 2200 MPa (ISO 178, 2 mm/min)
Impact Properties
  • Izod Notched Impact Strength: 22 kJ/m² (ISO 180/1A, at 23°C, 5.5J)
Thermal Properties
  • Heat Deflection Temperature (HDT): 82°C (ISO 75-2/A, at 1.8 MPa)
  • Vicat Softening Temperature: 103°C (ISO 306, 50N, 50°C/h)
Process Guide
  • Drying Recommendation: Pre-dry at 80°C for 2–4 hours in an air-circulating oven if no venting.
  • Melt Temperature Range: 190–230°C

Features & Benefits

Medium-High Heat Resistance

With a Heat Deflection Temperature (HDT) of 82°C (ISO 75-2/A) and Vicat Softening Temperature of 103°C, Eastech B532E is ideal for demanding applications such as refrigeration units and automotive parts.

Excellent Surface Finish

This ABS resin offers superior surface smoothness, enabling high-quality finishes with consistent aesthetics. This quality is essential for industries like furniture manufacturing, where polished appearances matter.

Balanced Rigidity and Toughness

Eastech B532E provides an ideal balance of 48 MPa tensile strength and 15% elongation at break (ISO 527). This makes it suitable for applications requiring durability, like extrusion and co-extrusion of thick sheets for packaging and sanitary products.

shandong eastech abs resin 25kg package

Use & Applications

  • Refrigeration: Durable, heat-resistant components for cooling systems.
  • Automotive: Functional interior and exterior profiles with excellent dimensional stability.
  • Hygiene: High-stretch ratio materials for sanitary applications.
  • Packaging & Furniture: Co-extruded sheets with uniform surfaces for high-end consumer products.