Plastic Granules
Eastech E332 Injection Grade/Extrusion Grade
Eastech E332 is an injection/extrusion-grade ABS resin that excels in fluidity, impact resistance, and thermal stability. Designed to streamline manufacturing processes, it is ideal for automotive interior components, electrical parts, and material modification applications.
Typical property data
Physical Properties
- Density: 1.04 g/cm³ (ISO 1183, 23°C)
- Melt Mass-Flow Rate (MFR): 12 g/10 min (ISO 1133, 220°C/10 kg)
- Molding Shrinkage: 0.4–0.7% (ISO 294/4, 23°C)
Mechanical Properties
- Tensile Strength at Yield: 50 MPa (ISO 527, 50 mm/min)
- Tensile Elongation at Break: 15% (ISO 527, 50 mm/min)
- Tensile Modulus: 2450 MPa (ISO 527, 1 mm/min)
- Flexural Strength: 75 MPa (ISO 178, 2 mm/min)
- Flexural Modulus: 2300 MPa (ISO 178, 2 mm/min)
Impact Properties
- Izod Notched Impact Strength: 20 kJ/m² (ISO 180/1A, 23°C, 5.5J)
Thermal Properties
- Heat Deformation Temperature: 82°C (ISO 75-2/A, 1.8 MPa)
- Vicat Softening Temperature: 102°C (ISO 306, 50N, 50°C/h)
Process Guide
- Pre-Drying: 80°C for 2–4 hours in an air circulating oven (for both extrusion and injection molding).
- Melt Temperature: 190–230°C (Extrusion); 220–260°C (Injection Molding).
- Mold Temperature: 40–70°C (Injection Molding).
Features & Benefits
Medium-High Heat Resistance
Eastech E332 maintains excellent dimensional stability under high temperatures, making it perfect for demanding environments such as under-the-hood automotive parts and heat-sensitive electrical components.
Superior Processing Efficiency
With a melt mass-flow rate of 12 g/10 min, this ABS resin delivers smoother and faster injection/extrusion, allowing manufacturers to improve production rates and reduce downtime.
Balanced Strength and Impact
Offering 50 MPa tensile strength and 20 kJ/m² impact strength, Eastech E332 provides durability and toughness, ensuring longevity in end-use applications like automotive panels and protective casings.
Use & Applications
- Automotive Components: Perfect for durable, heat-resistant interior parts like dashboards, consoles, and trims.
- Electrical Industry: Reliable material for sturdy casings, connectors, and other components requiring insulating properties.
- Material Modification: Versatile for blending with plastics, expanding its utility across multiple industrial applications.