Eastech Chemical M4 ABS

shandong eastech abs resin 25kg package

Eastech M4 Matte Extrusion Grade High Stretch Ratio

Eastech M4 is a matte extrusion-grade ABS resin featuring a high stretch ratio and a smooth surface. Designed for modern manufacturing needs, it offers exceptional mechanical properties and thermal stability, making it ideal for industries like automotive, construction, and sheet fabrication.

Associated Documents

TDS - Data Sheet
ABS SVHC
ABS FDA
ABS ROHS
ABS TSCA
ABS POPs
ABS PAHs

Typical property data

Physical Properties
  • Density: 1.04 g/cm³ (ISO 1183, 23 °C)
  • Melt Mass-Flow Rate (MFR): 9 g/10 min (ISO 1133, 220 °C/10 kg)
  • Molding Shrinkage: 0.4–0.7% (ISO 294/4, 23 °C)
Mechanical Properties
  • Tensile Strength at Yield: 35 MPa (ISO 527, 50 mm/min)
  • Tensile Elongation at Break: 80% (ISO 527, 50 mm/min)
  • Tensile Modulus: 1400 MPa (ISO 527, 1 mm/min)
  • Flexural Strength: 46 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 1500 MPa (ISO 178, 2 mm/min)
Impact Properties
  • Izod Notched Impact Strength: 10 kJ/m² (ISO 180/1A, 23 °C, 5.5 J)
Thermal Properties
  • Heat Deformation Temperature: 77 °C (ISO 75-2/A, 1.8 MPa)
  • Vicat Softening Temperature: 101 °C (ISO 306, 50 N, 50 °C/h)
Optical Properties
  • Glossiness: 10° GU (ASTM D523-14, 60°)
Process Guide
  • Pre-Drying: 80 °C for 2–4 hours in an air-circulating oven (if no venting)
  • Melt Temperature: 180–220 °C

Features & Benefits

Matte Finish for Premium Aesthetics

The matte surface finish ensures a refined, non-glossy appearance, perfect for visible components like automobile interiors and decorative panels.

High Stretch Ratio for Durability

With an elongation at break of up to 80%, Eastech M4 ensures improved tensile performance, allowing products like molded parts and co-extruded sheets to endure long-term wear and stress with reliability.

Thermal Stability for Versatile Applications

Eastech M4 offers excellent thermal characteristics, including a Vicat softening temperature of 101°C and heat deformation resistance at 77°C. This makes it highly suitable for applications requiring stability under elevated operational temperatures.

shandong eastech abs resin 25kg package

Use & Applications

  • Automotive & Transportation: Ideal for lightweight yet durable interior and exterior components.
  • Extruded or Co-Extruded Sheets: Perfect for packaging, appliance covers, and construction materials.
  • Modified Products: Adaptable for blends or specialty formulations tailored to unique end-product demands.
shandong eastech abs resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.