Physical Properties
- Melt Flow Index: 27 g/10 min (ISO 1133, 300°C × 1.2 kg)
- Specific Gravity: 1.2 (ISO 1183, 23°C)
Mechanical Properties
- Tensile Strength: 60 MPa (ISO 527, 23°C, 50 mm/min)
- Flexural Strength: 100 MPa (ISO 178, 23°C, 2 mm/min)
- Flexural Modulus: 2230 MPa (ISO 178, 23°C, 2 mm/min)
- Rockwell Hardness: R-122 (ISO 2039-2, 23°C)
Thermal Properties
Heat Deflection Temperature: 125°C (ISO 75/A, unannealed, 1.8 MPa, 4 mm, 120°C/h)
Other Properties
- Molding Shrinkage: 0.5–0.7% (ISO 2577)
- Light Transmission: Not specified fully in the parsed text (ISO 13468-1)
- Combustibility: UL 94 V-2, 0.75 mm (UL-94)
Features & Benefits
Superior Light Diffusion
TAIRILITE AC2856 scatters light uniformly (89–91% haze), eliminating hotspots in lampshades and bulbs. This ensures consistent illumination without costly secondary treatments.
Optimized Molding Efficiency
With a melt flow index of 27 g/10 min, it fills complex molds rapidly. Reduce cycle times and energy costs while maintaining part integrity—ideal for high-volume production.
UV Resistance for Longevity
Rated “f1” per UL 746C, it withstands outdoor UV exposure, water, and heat (RTI up to 130°C). Prevents yellowing/cracking, extending product life in harsh environments.