Typical property data

Physical Properties
  • Melt Flow Index (MFI): 10 g/10 min (ISO 1133, 300°C × 1.2 kg)
  • Specific Gravity: 1.19 (ISO 1183, 23°C/23°C)
Mechanical Properties
  • Tensile Strength: 67 MPa (ISO 527, 23°C)
  • Flexural Strength: 99 MPa (ISO 178, 23°C)
  • Flexural Modulus: 2150 MPa (ISO 178, 23°C)
  • Rockwell Hardness: R-122 (ISO 2039-2, 23°C)
Impact Properties
  • IZOD Impact Strength: 735 J/m (ISO 180, 23°C, 3.2 mm)
Thermal Properties
  • Heat Deflection Temperature (HDT): 113°C (ISO 75/A, Unannealed, 1.8 MPa, 3.2 mm)
Flame Characteristics
  • Combustibility (UL-94):
  • V-0 (1–3 mm thickness)
  • V-1 (0.8 mm thickness)
  • V-2 (0.6 mm thickness)
Injection Molding
  • Molding Shrinkage: 0.5%–0.7% (FCFC Method, 23°C)

Use & Applications

Transformer Cases

Flame-retardant protection for electrical insulation.

Battery Enclosures

Impact-resistant safety for EV/power storage systems.

Projector Housings

Precision molding for complex optical equipment.

Electromechanical Covers

Durability in industrial machinery and IoT devices.

tairilite pc resin

Features & Benefits

Halogen-Free Flame Retardancy

AC3610-AF achieves UL94 V-0 fire resistance (1–3 mm thickness) without toxic halogens or antimony. Ensures safety in electrical components while meeting eco-friendly regulations.

Superior Impact Resistance

With 735 J/m Izod impact strength (ISO 180), it withstands drops and shocks in rugged environments, reducing part failures in automotive or industrial housings.

High-Flow Processing Efficiency

Melt flow index of 10 g/10 min (ISO 1133) enables easy filling of intricate molds, cutting cycle times and production costs for complex geometries.

tairilite pc resin

FAQs

Is AC3610-AF halogen-free?

The ISO TDS lists “Cl, Br, Sb free” in the features, not the exact term “halogen-free.” A current RoHS/halogen report was not provided; confirm before making a halogen-free claim.

What UL94 coverage does AC3610-AF have?

UL Product iQ for AC361x lists V-2 at 0.6 mm, V-1 at 0.8 mm, V-0 at 1.0–3.0 mm, and 5VB at 2.0–3.0 mm, in ALL colors. The ISO TDS lists V-0 1–3 mm, V-1 0.8 mm, and V-2 0.6 mm. Verify the exact thickness and color you need.

Does AC3610-AF have UL 746C f1 outdoor suitability?

The provided UL excerpt does not list UL 746C f1 for AC3610-AF. For outdoor use, request the current UL Product iQ page or consider f1-rated grades.

What processing window is recommended for AC3610-AF?

The processing guide recommends pre-drying at 110–120°C for 4–6 hr. Screw temperature is 260–295°C, mold temperature 80–100°C, and injection pressure 50–130 kg/cm². Confirm with your machine and mold.

What are the special features of AC3610-AF?

It is a high-flow, non-transparent, flame-retardant grade with Cl, Br, Sb free formulation. It is often used where halogen-free alternatives are preferred and high flow is needed.

AC3610-AF Related Flame Retardant Grades

Disclaimer:Disclaimer: The grades below are potential alternatives for comparison only from FORMOSA (FCFC). They are not direct drop-in replacements. UL ratings are color- and thickness-dependent. Typical values are not specifications. All property data is from ISO TDS unless otherwise stated. Please verify current UL Product iQ status, request TDS/SDS/COA and test samples before substitution.

Grade / Manufacturer Positioning vs. AC3610-AF UL94 (ISO TDS) MFR HDT Notched Impact (IZOD / Charpy) Color UV / UL 746C f1
AC3600
FORMOSA TAIRILITE® PC
Identical UL94 coverage, upgraded to high heat resistance (HDT 123 °C), labeled halogen-free V-2 0.6 mm; V-1 0.8 mm; V-0 1.0–3.0 mm; 5VB 2.0–3.0 mm 11 g/10 min 123 °C IZOD 735 J/m; Charpy 65 kJ/m² Non-transparency; ALL /
AC3710
FORMOSA TAIRILITE® PC
High-flow (MFR 28) sister for thin-wall molding; same halogen-free non-transparent FR V-1 0.45 mm; V-0 0.6–3.0 mm; 5VB 1.5–3.0 mm 28 g/10 min N/A (ISO TDS value anomalous) IZOD 685 J/m; Charpy 40 kJ/m² Non-transparency; ALL /
AC3630
FORMOSA TAIRILITE® PC
High-flow non-transparent FR upgraded with UL weather resistance / 746C f1 V-0 0.8–3.0 mm; 5VB 1.5–3.0 mm 25 g/10 min N/A (ISO TDS value anomalous) IZOD 635 J/m; Charpy 55 kJ/m² Non-transparency; ALL UL weather / UL 746C f1

↩ Back to FORMOSA (FCFC) Flame Retardant PC Resin Hub (13 grades)

Substitution checklist: Before replacing any grade, verify UL94 at the same wall thickness, UL-listed color, halogen-free declaration, MFR/MVR, HDT, notched impact, UV / UL 746C f1 and processing window.

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.