Formosa (FCFC) TAIRILITE® AC3630

TAIRILITE® AC3630 PC Resin Self Extinguishing Grade

Tairilite AC3630 is a self-extinguishing grade Polycarbonate PC Resin. Combining halogen-free flame retardancy, high flow, non-transparency, and UL weather resistance certification, it delivers unmatched safety and durability. Ideal for industries prioritizing reliability and compliance.

tairilite pc resin

Download PDF

ISO Data Sheet
ASTM Data Sheet

Typical property data

Physical Properties
  • Melt Flow Index: 25 g/10 min (ISO 1133, 300℃ × 1.2kg)
  • Specific Gravity: 1.19 (ISO 1183, 23℃/23℃)
Mechanical Properties
  • Tensile Strength: 66 MPa (ISO 527, 23℃)
  • Flexural Strength: 106 MPa (ISO 178, 23℃)
  • Flexural Modulus: 2350 MPa (ISO 178, 23℃)
  • IZOD Impact Strength: 635 J/m (ISO 180, 23℃, 3.2mm)
  • Charpy Impact Strength: 55 kJ/m² (ISO 179, 23℃, 4mm)
  • Rockwell Hardness: R-121 (ISO 2039-2, 23℃)
Thermal Properties
  • Vicat Softening Point: 116℃ (ISO 306, VICAT(10N))
  • Heat Deflection Temperature: 0.45℃ (ISO 75/A, Unannealed, 18.6 kg/cm², 1.8MPa, 3.2mm)
Flame Characteristics
  • UL-94: V-0 (0.8 ~ 3 mm), 5VB (1.5 ~ 3 mm)
Injection Molding
  • Molding Shrinkage: 0.5 ~ 0.7% (ISO 2577, 3.2mm)

Features & Benefits

Superior Flame Retardancy

Halogen-free and UL94 V-0/5VB rated, AC3630 eliminates toxic fumes during combustion. This ensures safer electronics and compliance with global environmental regulations.

High-Flow Processing Efficiency

With a melt flow index of 25 g/10 min, it fills complex molds effortlessly. Reduces cycle times and energy costs while minimizing defects in thin-walled parts.

Weather-Resistant Durability

UL-certified for outdoor use, it withstands UV exposure and temperature swings. Non-transparent properties prevent degradation, ideal for long-lasting outdoor equipment.

tairilite pc resin

Use & applications

Household appliances

Flame-retardant housings for heaters/irons.

3C electronics

Laptop casings and power adapters.

Outdoor equipment

UV-resistant drone/controller shells.

E-bike battery cases

Impact protection for lithium packs.

Energy storage

Robust enclosures for solar battery systems.

tairilite pc resin ac3630 application

FAQs

Is AC3630 halogen-free?

The supplied ISO TDS lists “Halogen free” in the features.

Does AC3630 have UL 746C f1 outdoor suitability?

The ISO TDS lists “UL weather resistance certification,” but a UL 746C f1 listing was not provided. For outdoor use, request the current UL Product iQ page or consider grades with explicit f1 coverage.

What UL94 coverage does AC3630 have?

The ISO TDS lists V-0 at 0.8–3.0 mm and 5VB at 1.5–3.0 mm. A UL Product iQ yellow card was not provided in the supplied documents. Verify the current UL status and color coverage before design freeze.

What are the special features of AC3630?

It is a high-flow, non-transparent, halogen-free flame-retardant grade with UL weather resistance certification. It is often used for outdoor or weather-exposed parts requiring high flow.

AC3630 Related Flame Retardant Grades

Disclaimer:Disclaimer: The grades below are potential alternatives for comparison only from FORMOSA (FCFC). They are not direct drop-in replacements. UL ratings are color- and thickness-dependent. Typical values are not specifications. All property data is from ISO TDS unless otherwise stated. Please verify current UL Product iQ status, request TDS/SDS/COA and test samples before substitution.

Grade / Manufacturer Positioning vs. AC3630 UL94 (ISO TDS) MFR HDT Notched Impact (IZOD / Charpy) Color UV / UL 746C f1
AC3710
FORMOSA TAIRILITE® PC
Closest indoor sister: same high-flow non-transparent FR, without the UL weather / f1 package V-1 0.45 mm; V-0 0.6–3.0 mm; 5VB 1.5–3.0 mm 28 g/10 min N/A (ISO TDS value anomalous) IZOD 685 J/m; Charpy 40 kJ/m² Non-transparency; ALL /
AC3610-AF
FORMOSA TAIRILITE® PC
Lower-flow non-transparent FR with explicit Cl / Br / Sb-free; broader thin-wall UL coverage V-2 0.6 mm; V-1 0.8 mm; V-0 1.0–3.0 mm; 5VB 2.0–3.0 mm 10 g/10 min 113 °C IZOD 735 J/m Non-transparency; ALL /
AC3839
FORMOSA TAIRILITE® PC
UV+f1 outdoor alternative with low-temperature impact for cold-climate housings V-0 1.0–3.0 mm; 5VA 3.0 mm 12 g/10 min 125 °C Charpy 70 kJ/m² ALL UL 746C f1; UV resistance

↩ Back to FORMOSA (FCFC) Flame Retardant PC Resin Hub (13 grades)

Substitution checklist: Before replacing any grade, verify UL94 at the same wall thickness, UL-listed color, halogen-free declaration, MFR/MVR, HDT, notched impact, UV / UL 746C f1 and processing window.