TAIRILITE® AC3710 PC Resin Self Extinguishing Grade
TAIRILITE AC3710 is a halogen-free, flame-retardant polycarbonate resin combining high flow efficiency and non-transparency. This self-extinguishing grade excels in thin-walled applications like electronics and energy storage, delivering UL94 V-0 compliance, rapid molding, and robust impact resistance—ideal for safety-critical, high-performance components.
Plastic Granules
Download PDF
ISO Data Sheet
MSDS
UL Product iQ
Processing Data
Typical property data
Physical Properties
- Melt Flow Index: 28 g/10 min (ISO 1133, 300°C × 1.2kg)
- Specific Gravity: 1.2 (ISO 1183, 23°C/23°C)
Mechanical Properties
- Tensile Strength: 63 MPa (ISO 527, 23°C)
- Flexural Strength: 104 MPa (ISO 178, 23°C)
- Flexural Modulus: 2350 MPa (ISO 178, 23°C)
- Rockwell Hardness: R122 (R-scale, ISO 2039-2, 23°C)
Impact Properties
- IZOD Impact Strength: 685 J/m (ISO 180, 23°C, 3.2mm)
- Charpy Impact Strength: 40 kJ/m² (ISO 179, 23°C, 4mm)
Thermal Properties
- Vicat Softening Point: 120°C (ISO 306, VICAT 10N)
- Heat Deflection Temperature: 0.45°C (ISO 75/A, Unannealed, 18.6 kg/cm², 3.2mm)
Optical Properties
- Transparency: Non-transparent (specification feature)
Flame Characteristics
- Combustibility:
- UL-94 V-0 (0.6 ~ 3 mm)
- UL-94 V-1 (0.45 mm)
- UL-94 5VB (1.5 ~ 3 mm)
- Halogen-free, flame-retardant (specification feature)
Injection Molding
- Molding Shrinkage: 0.5 ~ 0.7% (ISO 2577, 3.2mm)
Use & Applications
- Thin-Walled Electronics Casings: Laptop battery housings, smartphone components, tablet frames.
- Energy Storage & EV Components: Battery module housings, EV charging connectors, power distribution units.
- Household Appliances: Power tool housings, kitchen appliance switches, air conditioner internal parts.
- Industrial Control Systems: Circuit breaker casings, control panel covers, sensor housings.
Features & Benefits
Self-Extinguishing Safety
Tairilite PC AC3710’s self-extinguishing grade eliminates halogen additives while achieving UL94 V-0 compliance (0.6–3mm thickness), ensuring fire-resistant housings for high-risk environments like battery casings and energy storage systems.
High Flow for Precision Molding
With a melt flow index of 28g/10min, this resin fills intricate, thin-walled molds effortlessly—perfect for compact 3C electronics (e.g., <1mm laptop battery covers) without compromising structural integrity.
Impact Resistance Under Stress
Boasting IZOD impact strength of 685 J/m and Charpy impact of 40 kJ/m², TAIRILITE AC3710 withstands drops, vibrations, and mechanical stress, ideal for rugged housings in appliances and industrial equipment.
FAQs
The ISO TDS lists “Cl, Br, Sb free” in the features, not the exact term “halogen-free.” A current RoHS/halogen report was not provided; confirm before making a halogen-free claim.
UL Product iQ for AC361x lists V-2 at 0.6 mm, V-1 at 0.8 mm, V-0 at 1.0–3.0 mm, and 5VB at 2.0–3.0 mm, in ALL colors. The ISO TDS lists V-0 1–3 mm, V-1 0.8 mm, and V-2 0.6 mm. Verify the exact thickness and color you need.
The provided UL excerpt does not list UL 746C f1 for AC3610-AF. For outdoor use, request the current UL Product iQ page or consider f1-rated grades.
The processing guide recommends pre-drying at 110–120°C for 4–6 hr. Screw temperature is 260–295°C, mold temperature 80–100°C, and injection pressure 50–130 kg/cm². Confirm with your machine and mold.
It is a high-flow, non-transparent, flame-retardant grade with Cl, Br, Sb free formulation. It is often used where halogen-free alternatives are preferred and high flow is needed.
AC3710 Related Flame Retardant Grades
Disclaimer:Disclaimer: The grades below are potential alternatives for comparison only from FORMOSA (FCFC). They are not direct drop-in replacements. UL ratings are color- and thickness-dependent. Typical values are not specifications. All property data is from ISO TDS unless otherwise stated. Please verify current UL Product iQ status, request TDS/SDS/COA and test samples before substitution.
| Grade / Manufacturer | Positioning vs. AC3710 | UL94 (ISO TDS) | MFR | HDT | Notched Impact (IZOD / Charpy) | Color | UV / UL 746C f1 |
|---|---|---|---|---|---|---|---|
| AC3630 FORMOSA TAIRILITE® PC | Same high-flow non-transparent FR, upgraded with UL weather resistance / 746C f1 for outdoor housings | V-0 0.8–3.0 mm; 5VB 1.5–3.0 mm | 25 g/10 min | N/A (ISO TDS value anomalous) | IZOD 635 J/m; Charpy 55 kJ/m² | Non-transparency; ALL | UL weather / UL 746C f1 |
| AC3610-AF FORMOSA TAIRILITE® PC | Lower-flow sister: non-transparent FR with explicit Cl / Br / Sb-free declaration | V-2 0.6 mm; V-1 0.8 mm; V-0 1.0–3.0 mm; 5VB 2.0–3.0 mm | 10 g/10 min | 113 °C | IZOD 735 J/m | Non-transparency; ALL | / |
| AC3600 FORMOSA TAIRILITE® PC | Lower-flow sister, upgraded to high heat resistance (HDT 123 °C) for adapters & transformers | V-2 0.6 mm; V-1 0.8 mm; V-0 1.0–3.0 mm; 5VB 2.0–3.0 mm | 11 g/10 min | 123 °C | IZOD 735 J/m; Charpy 65 kJ/m² | Non-transparency; ALL | / |