Plastic Granules
TAIRILITE® AC9140 PC Resin Ultra-low Temp Resistance Copolymer
TAIRILITE AC9140 is a premium polycarbonate raw material. Combining exceptional transparency (>87% transmission), mid-flow processability, and outstanding low-temperature impact resistance, this UV-stabilized material ensures reliability in high-performance 3C electronics and protective equipment. Ideal for buyers prioritizing durability and optical clarity.
Typical property data
Physical Properties
- Specific Gravity: 1.18 (ISO 1183, 23°C)
- Melt Flow Index: 13 g/10 min (ISO 1133, 300°C × 1.2 kg)
Mechanical Properties
- Tensile Strength: 60 MPa (ISO 527, 23°C, 50 mm/min)
- Flexural Strength: 98 MPa (ISO 178, 23°C, 2 mm/min)
- Flexural Modulus: 2060 MPa (ISO 178, 23°C, 2 mm/min)
- Rockwell Hardness: R-120 (ISO 2039-2, 23°C)
Impact Properties
- Charpy Impact Strength: 60 kJ/m² (ISO 179, 23°C, 4 mm, Notched)
Thermal Properties
- Heat Deflection Temperature: 120°C (ISO 75/A, Unannealed, 1.8 MPa, 4 mm, 120°C/h)
Optical Properties
- Transmission: > 87% (ISO 13468/1, 3.2 mm)
- Haze: < 1.0% (ISO 14782, 3.2 mm)
Flame Characteristics
- Combustibility: UL-94 V-2 (2 mm, File No. E162823)
Injection Molding
- Molding Shrinkage: 0.6–0.8% (ISO 2577)
Features & Benefits
Crystal-Clear Durability
TAIRILITE® PC Resin delivers >87% light transmission and <1.0% haze (ISO 13468/1), rivaling glass without brittleness. Perfect for scratch-resistant device screens and lenses.
Unmatched Impact Resilience
It withstands harsh environments (60 kJ/m² Charpy impact at 23°C, ISO 179), preventing brittle failures in sports gear or outdoor electronics in sub-zero conditions.
Safe & Stable Processing
UL-certified (RTI 80°C) and non-hazardous (SDS), it resists degradation below 320°C. Mid-flow MFI (13g/10min, ISO 1133) enables efficient molding of complex parts.
Use & applications
- 3C Electronics: Smartphone/tablet cases, laptop housings, wearables.
- Protective Gear: Safety goggles, helmets, sports equipment.