Plastic Granules
TAIRILITE® AC9144 PC Resin Ultra-low Temp Resistance Copolymer
TAIRILITE AC9144 by FCFC is a high-performance PC resin. Combining translucency, mid-flow processing, low-temperature impact strength, and UV resistance, this material delivers exceptional durability and versatility. Ideal for precision-molded components where reliability matters most.
Associated Documents
ISO Data Sheet
ASTM Data Sheet
MSDS
Processing Data
Typical property data
Physical Properties
- Melt Flow Index: 13 g/10 min (ISO 1133, 300°C, 1.2 kg)
- Specific Gravity: 1.18 (ISO 1183, 23°C)
Mechanical Properties
- Tensile Strength: 60 MPa (ISO 527, 23°C, 50 mm/min)
- Flexural Strength: 98 MPa (ISO 178, 23°C, 2 mm/min)
- Flexural Modulus: 2060 MPa (ISO 178, 23°C, 2 mm/min)
- Rockwell Hardness: R-120 (ISO 2039-2, 23°C)
Thermal Properties
- Heat Deflection Temperature: 120°C (ISO 75/A, unannealed, 1.8 MPa, 4 mm, 120°C/h)
Optical Properties
- Features: Translucency
Flame Characteristics
- Combustibility: V-2 (UL-94, 2 mm)
Injection Molding
Molding Shrinkage: 0.6–0.8% (ISO 2577)
Features & Benefits
Superior Impact Resistance
TAIRILITE AC9144 maintains exceptional toughness even in freezing conditions (-40°C), preventing cracks in sports gear or outdoor equipment. Ideal for protective helmets or rugged 3C casings.
Enhanced UV Protection & Clarity
Built-in UV resistance prevents yellowing and degradation in sunlight, ensuring long-term aesthetics for consumer electronics like smartphone covers or transparent displays.
Optimized Flow for Complex Molds
Mid-flow properties enable seamless filling of intricate designs, reducing defects in thin-walled laptop housings or sports equipment components.
Use & applications
- 3C Electronics: Smartphone/tablet cases, laptop housings, wearables.
- Sports & Safety: Bicycle helmets, protective goggles, ski gear.
- Outdoor Equipment: Durable components for UV-exposed tools or enclosures.