Plastic Granules
TARFLON™ A2200 Natural Color Injection Molding
Tarflon A2200 is a high-performance polycarbonate resin designed for injection molding and compounding. Combining exceptional impact resistance, thermal stability, and electrical insulation, it’s ideal for automotive, electronics, and industrial components. With natural color versatility and UL-certified safety, Tarflon A2200 delivers reliability in demanding environments while streamlining production efficiency.
Associated Documents
Data Sheet
Typical property data
Physical Properties
- MFR (Melt Flow Rate): 11 g/10min (ISO 1133)
- Density: 1.2 g/cm³ (ISO 1183)
- Water Absorption (50%RH, 24hr): 0.23% (ISO 62)
Mechanical Properties
- Tensile Stress at Yield: 65 MPa (ISO 527-1,2)
- Tensile Strain at Break: 95% (ISO 527-1,2)
- Flexural Strength: 90 MPa (ISO 178)
- Flexural Modulus: 2.3 GPa (ISO 178)
- Rockwell Hardness: R120/M50 (ISO 2039-2)
Impact Properties
- Charpy Impact Strength (Notched): 80 kJ/m² (ISO 179-1)
Thermal Properties
- Heat Deflection Temperature (1.8 MPa): 125°C (ISO 75-1,2)
- Linear Thermal Expansion Coefficient: 6.5 × 10⁻⁵ /°C (ISO 11359-2)
Optical Properties
- Total Luminous Transmittance: 85–90% (ISO 13468-1)
Electrical Properties
- Dielectric Strength: 30 kV/mm (IEC 60243-1)
- Volume Resistivity: >10¹⁶ Ω·cm (ASTM D257)
- Dielectric Constant (1 MHz): 2.85 (IEC 60250)
- Dielectric Dissipation Factor (1 MHz): 0.0092 (IEC 60250)
Flame Characteristics
- Flammability Rating (UL94):
- V-2 (0.36–2.9 mm thickness)
- HB (3.0–6.0 mm thickness)
- Comparative Tracking Index (CTI): PLC level 2 (UL746A)
- Relative Temperature Index (RTI):
- Electrical: 130°C (UL746B)
- Impact: 125°C (UL746B)
- Strength: 130°C (UL746B)
- UV/Water Exposure Resistance: f2 rating (UL746C)
Injection Molding
- Pre-drying Condition: 120°C, 5–8 hours
- Cylinder Temperature: 260–300°C (Max. 320°C)
- Mold Temperature: 80–120°C
Features & Benefits
Unmatched Impact Resistance
With a Charpy impact strength of 80 kJ/m², Tarflon A2200 withstands high-stress environments, reducing part failure in automotive bumpers or protective equipment.
Heat-Resistant Durability
A heat deflection temperature of 125°C ensures stability in high-temperature applications like electronic housings or under-the-hood automotive components.
Superior Electrical Safety
Dielectric strength (30 kV/mm) and volume resistivity (>10¹⁶ Ω·cm) make it perfect for circuit breakers, connectors, and UL-rated industrial controls.
Use & Applications
- Injection molded parts requiring high clarity and strength
- Compounded materials for custom formulations
- Transparent housings for consumer electronics
- Automotive interior or lighting components
- Medical device casings and enclosures
- High-performance industrial equipment covers