Plastic Granules
TARFLON™ HQ2200 Clean Grade Film Grade LCD Film Printing
Tarflon HQ2200 is a high-performance polycarbonate resin engineered for precision and durability. With exceptional impact resistance, high tensile strength, and excellent optical clarity, it’s ideal for demanding applications like high-quality films, printing surfaces, and components requiring low contamination.
Associated Documents
Data Sheet
Typical property data
Physical Properties
- MFR (Melt Flow Rate): 11 g/10min (ISO 1133)
- Density: 1.2 g/cm³ (ISO 1183)
- Water Absorption (50%RH, 24hr): 0.23% (ISO 62)
Mechanical Properties
- Tensile Stress at Yield: 65 MPa (ISO 527-1,2)
- Tensile Strain at Break: 95% (ISO 527-1,2)
- Flexural Strength: 90 MPa (ISO 178)
- Flexural Modulus: 2.3 GPa (ISO 178)
- Rockwell Hardness: R120/M50 (ISO 2039-2)
Impact Properties
- Charpy Impact Strength (Notched): 80 kJ/m² (ISO 179-1)
Thermal Properties
- Heat Deflection Temperature (1.8 MPa): 125°C (ISO 75-1,2)
- Linear Thermal Expansion Coefficient: 6.5 × 10⁻⁵ /°C (ISO 11359-2)
- Mold Shrinkage: 0.5 ~ 0.7% (ASTM D955)
Optical Properties
- Total Luminous Transmittance: 85 ~ 90% (ISO 13468-1)
Electrical Properties
- Dielectric Strength: 30 kV/mm (IEC 60243-1)
- Volume Resistivity: >10¹⁶ Ω·cm (ASTM D257)
- Dielectric Constant (1 MHz): 2.85 (IEC 60250)
- Dielectric Dissipation Factor (1 MHz): 0.0092 (IEC 60250)
Injection Molding
- Pre-Drying Condition: 120°C, 5 ~ 8 hours
- Cylinder & Die Temperature: 240 ~ 290°C
- Roll Temperature: 120 ~ 145°C
Features & Benefits
High Impact Resistance
Tarflon HQ2200 delivers 80 kJ/m² Charpy impact strength, reducing breakage in rugged environments. Perfect for automotive interior panels or protective electronic housings that endure drops or vibrations.
Superior Optical Clarity
With 85–90% luminous transmittance, this resin ensures crystal-clear visibility. Ideal for LED light diffusers, medical device windows, or glossy packaging films where visual appeal matters.
Thermal & Dimensional Stability
A heat deflection temperature of 125°C and low mold shrinkage (0.5–0.7%) guarantee consistent performance under heat and pressure. Use it for precision-molded parts like connectors or industrial tooling.
Use & Applications
- High-Clarity Films: Packaging films, display covers, or decorative laminates with minimal contamination.
- Printing & Electronics: Printer components, touchscreen layers, or LED light guides requiring scratch resistance.
- Medical & Food-Grade Parts: Transparent housings or containers where cleanliness and durability are critical.