Typical property data

Physical Properties
  • Melt Flow Rate (MFR): 26 g/10min (ISO 1133)
  • Density: 1.2 g/cm³ (ISO 1183)
  • Water Absorption (50%RH 24hr): 0.23% (ISO 62)
Mechanical Properties
  • Tensile Stress at Yield: 65 MPa (ISO 527-1,2)
  • Tensile Strain at Break: 95% (ISO 527-1,2)
  • Flexural Strength: 90 MPa (ISO 178)
  • Flexural Modulus: 2.3 GPa (ISO 178)
  • Rockwell Hardness: R120/M50 (ISO 2039-2)
Impact Properties

Charpy Impact Strength (Notched): 40 kJ/m² (ISO 179-1)

Thermal Properties
  • Heat Deflection Temperature (1.8 MPa): 125°C (ISO 75-1,2)
  • Linear Thermal Expansion Coefficient: 6.5×10−56.5 \times 10^{-5}/°C (ISO 11359-2)
  • Mold Shrinkage: 0.5–0.7% (ASTM D955)
Optical Properties

Total Luminous Transmittance: 85–90% (ISO 13468-1)

Electrical Properties
  • Dielectric Strength: 30 kV/mm (IEC 60243-1)
  • Volume Resistivity: > 101610^{16} Ω·cm (ASTM D257)
  • Dielectric Constant (1 MHz): 2.85 (IEC 60250)
  • Dielectric Dissipation Factor (1 MHz): 0.0092 (IEC 60250)
Flame Characteristics
  • UL Flammability Rating:
    • V-2 (0.36–2.4 mm) (UL94)
    • HB (2.5–6.0 mm) (UL94)
  • Comparative Tracking Index (CTI): PLC Level 2 (UL746A)
  • Relative Thermal Index (RTI):
    • Electrical: 130°C (UL746B)
    • Impact: 125°C (UL746B)
    • Strength: 130°C (UL746B)
  • UV and Water Exposure or Immersion: f2 (UL746C)
Injection Molding
  • Pre-drying Condition: 120°C, 5–8 hours
  • Cylinder Temperature: 260–300°C (Max 320°C)
  • Mold Temperature: 80–120°C

Features & Benefits

Unmatched Impact Resistance

Tarflon IR1700 delivers the highest Charpy impact strength (40 kJ/m²) among plastics, ensuring components like explosion-proof gloves or relay cases withstand harsh impacts without cracking.

Crystal-Clear Transparency

With 85-90% light transmittance, this resin maintains optical clarity even after molding—ideal for decorative lighting covers, safety lamps, or contact lens cases requiring both aesthetics and durability.

UL-Certified Safety & Stabilitylity

Compliant with UL94 V-2 and HB flammability ratings, Tarflon IR1700 ensures safety in electrical equipment while offering thermal stability (heat deflection up to 125°C) for high-temperature applications.

fipc tarflon ir1700

Use & Applications

  • Electrical & Safety: Relay cases, timer enclosures, explosion-proof gloves.
  • Consumer Goods: Dishes, cups, and glasses (NSF-certified for food contact).
  • Lighting & Optics: Decorative covers, safety lamps, UV-resistant contact lens cases.
  • Industrial Equipment: High-precision packs, machinery components requiring dimensional stability.