TARFLON™ IV1900R PC Resin Weathering Grade UV-stabilized

Tarflon IV1900R is a UV-stabilized polycarbonate resin offering exceptional clarity, durability, and mold release properties. Ideal for automotive and outdoor applications, it combines high impact resistance (70 kJ/m²), UV protection (cut-off <380 nm), and compliance with AMECA and UL f1 standards, ensuring reliability in harsh environments.

Associated Documents

Data Sheet

Typical property data

Physical Properties
  • Melt Flow Rate (MFR): 19 g/10min (ISO 1133)
  • Density: 1.2 g/cm³ (ISO 1183)
  • Water Absorption (50% RH, 24 hrs): 0.23% (ISO 62)
Mechanical Properties
  • Tensile Stress at Yield: 65 MPa (ISO 527-1,2)
  • Tensile Strain at Break: 95% (ISO 527-1,2)
  • Flexural Strength: 90 MPa (ISO 178)
  • Flexural Modulus: 2.3 GPa (ISO 178)
  • Charpy Impact Strength (Notched): 70 kJ/m² (ISO 179-1)
  • Rockwell Hardness (R/M Scale): R120/M50 (ISO 2039-2)
Impact Properties
  • Charpy Impact Strength (Notched): 70 kJ/m² (ISO 179-1)
Thermal Properties
  • Heat Deflection Temperature (HDT, 1.8 MPa): 125°C (ISO 75-1,2)
  • Linear Thermal Expansion Coefficient: 6.5×10−56.5 \times 10^{-5} /°C (ISO 11359-2)
  • Relative Thermal Index (RTI, Electrical): 130°C (UL746B)
  • RTI (Impact/Mechanical): 125°C (UL746B)
Optical Properties
  • Total Luminous Transmittance: 85–90% (ISO 13468-1)
Electrical Properties
  • Dielectric Strength: 30 kV/mm (IEC 60243-1)
  • Dielectric Constant (1 MHz): 2.85 (IEC 60250)
  • Dielectric Dissipation Factor (1 MHz): 0.0092 (IEC 60250)
Flame Characteristics
  • Flammability (UL94):
    • V-2 for 0.36–1.8 mm
    • HB for 1.9–6.0 mm
  • Comparative Tracking Index (CTI): PLC Level 2 (UL746A)
  • UV/Water Resistance: Rated f1 (UL746C)
Injection Molding Parameters
  • Pre-Drying Condition: 120°C for 5–8 hours
  • Cylinder Temperature: 260–300°C (Max. 320°C)
  • Mold Temperature: 80–120°C

Features & Benefits

Superior UV Resistance & Clarity

Tarflon IV1900R blocks harmful UV rays below 380 nm while maintaining 85–90% light transmittance. This ensures long-term color stability and prevents yellowing, perfect for automotive headlamps and outdoor lighting exposed to sunlight.

High Impact Strength

With a Charpy impact strength of 70 kJ/m², this Tarflon polycarbonate resists cracking under stress, reducing failure risks in components like vehicle housings or rugged outdoor equipment.

Efficient Mold Release

The resin’s excellent flow (MFR 19 g/10min) and low mold shrinkage (0.5–0.7%) streamline production, cutting cycle times and costs for high-volume parts like lenses or enclosures.

fipc tarflon™ pc resin 25kg package

Use & Applications

  • Automotive Lighting: AMECA-certified for headlamps, fog lights, and signal covers.
  • Outdoor Equipment: UV-resistant enclosures for LED streetlights or solar panels.
  • Industrial Components: High-impact housings for machinery and electrical systems.
  • Consumer Electronics: Durable, clear covers for displays or touchscreens.
tarflon iv1900r pc resin application

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.