Plastic Granules
TAIRILAC® AG16A1 ABS Resin Health Care Grade
Formosa ABS Tairilac AG16A1 is a healthcare-grade ABS resin engineered for precision medical applications. With high rigidity and medium impact strength, it delivers exceptional mechanical stability and biocompatibility, meeting stringent USP Plastic Class VI requirements. Ideal for critical healthcare components.
Download PDF
ISO TDS
ASTM TDS
SDS
UL Product iQ
Processing Data
Typical property data
Physical Properties
- Melt Flow Index:
- 1 g/10 min (ISO 1133, 200℃ × 5 kg)
- 11 g/10 min (ISO 1133, 220℃ × 10 kg)
- Specific Gravity: 1.04 (ISO 1183, 23 ℃/23 ℃)
Mechanical Properties
- Tensile Strength: 47 Mpa (ISO 527, 23 ℃, 50 mm/min)
- Flexural Strength: 72 Mpa (ISO 178, 23 ℃, 2 mm/min)
- Flexural Modulus: 2300 Mpa (ISO 178, 23 ℃, 2 mm/min)
- Rockwell Hardness: R-111 (ISO 2039-2, 23 ℃)
Impact Properties
- Charpy Impact Strength: 33 kJ/m² (ISO 179, 23 ℃, 4 mm thick, Notched)
Thermal Properties
- Vicat Softening Point: 94 ℃ (ISO 306, Annealed, 50N, 50℃/h)
- Heat Deflection Temperature: 88 ℃ (ISO 75/A, Annealed, 1.8 Mpa, 4 mm thick, 120℃/h)
Flame Characteristics
- Combustibility (UL-94): HB, 1.5 ~ 3 mm thickness (File No. E162823)
Injection Molding
- Molding Shrinkage: 0.4 ~ 0.7% (ISO 2577, 3.2 mm)
Use & Applications
Surgical Instruments
Scalpel shanks requiring rigidity and autoclave resistance.
Respiratory Devices
Asthma inhaler housings compliant with medical-grade standards.
Healthcare Components
IV connectors, diagnostic housings, and lab equipment.
Features & Benefits
Medical Safety Compliance
Certified USP Class VI biocompatible and UL94 HB flammability rated (1.5–3 mm), ensuring safety for skin-contact devices. Reduces regulatory hurdles for medical approvals.
Processing Efficiency
Low pre-drying needs (70–80°C × 2–3 hrs) and consistent mold shrinkage (0.4–0.7%). Streamlines production and minimizes defects in thin-walled parts.
Balanced Performance
High tensile strength (47 MPa) and impact resistance (33 kJ/m² Charpy). Withstands sterilization and daily wear in demanding medical environments.