TAIRILAC® AG23AT Electroplating Grade ABS Resin

Tairilac® AG23AT ABS Resin is a high-impact, electroplating-grade thermoplastic in natural color. Designed for demanding applications, it delivers exceptional surface finish for metallization, durability, and ease of processing—ideal for automotive, consumer goods, and industrial components.

Download PDF

ISO Data Sheet
ASTM Data Sheet
Material SDS
UL Product iQ
Processing Data

Typical property data

Physical Properties
  • Specific Gravity: 1.04 (ISO 1183, 23℃)
  • Melt Flow Index:
    • 2 g/10 min (ISO 1133, 200℃ × 5kg)
    • 20 g/10 min (ISO 1133, 220℃ × 10kg)
Mechanical Properties
  • Tensile Strength: 44 MPa (ISO 527, 23℃, 50mm/min)
  • Flexural Strength: 62 MPa (ISO 178, 23℃, 2mm/min)
  • Flexural Modulus: 2000 MPa (ISO 178, 23℃, 2mm/min)
Impact Properties
  • Charpy Impact Strength: 33 kJ/m² (ISO 179, 23℃, 4mm thick, Notched)
Thermal Properties
  • Vicat Softening Point: 94℃ (ISO 306, Annealed, 50N, 50℃/h)
  • Heat Deflection Temperature: 93℃ (ISO 75/A, Annealed, 1.8 MPa, 4mm thick, 120℃/h)
Flame Characteristics
  • Combustibility: HB for 1.5-3mm (UL-94, File No. E162823)
Injection Molding
  • Molding Shrinkage: 0.4–0.7% (ISO 2577, 3.2mm)

Use & Applications

  • Automotive: Wheel covers, door handles, chrome-plated trims.
  • Consumer Goods: Knobs, appliance tags, cosmetic packaging.
  • Industrial: Electroplated housings, tool grips, decorative fixtures.
  • Hardware: Bathroom faucets, cabinet pulls, and luxury accessories.
formosa plastics tairilac abs

Features & Benefits

Superior Electroplating Performance

AG23AT ensures flawless chrome adhesion and mirror-like finishes, critical for premium aesthetic parts like automotive grilles and faucets. Reduces rework and enhances product value.

High Impact Resistance

With 33 kJ/m² Charpy impact strength (ISO 179), it withstands drops and impacts in harsh environments—perfect for tool handles, knobs, and protective covers.

Easy Processing & Stability

It pre-dries quickly (70–80°C/2–3 hrs), processes at 190–230°C, and offers low mold shrinkage (0.4–0.7%). Simplifies production while minimizing warpage.

formosa plastics tairilac abs

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.