Physical Properties
  • Melt Flow Index (MFI): 10 g/10 min (ISO 1133, 200℃ × 5 kg)
  • Specific Gravity: 1.05 (ISO 1183, 23℃/23℃)
Mechanical Properties
  • Tensile Strength: 29 MPa (ISO 527, 23℃, 50 mm/min)
  • Flexural Strength: 41 MPa (ISO 178, 23℃, 2 mm/min)
  • Flexural Modulus: 1400 MPa (ISO 178, 23℃, 2 mm/min)
  • Charpy Impact Strength: 11 kJ/m² (ISO 179, 23℃, 4 mm thick, Notched)
Thermal Properties
  • Vicat Softening Point: 87 ℃ (ISO 306, Annealed, 50N, 50℃/h)
  • Heat Deflection Temperature (HDT): 88 ℃ (ISO 75/A, Annealed, 1.8 MPa, 4 mm thick, 120℃/h)
Other Properties
  • Molding Shrinkage: 0.4% ~ 0.7% (ISO 2577, 3.2 mm thick)
  • Features: Excellent weather resistance, suitable for modified plastic roof tile applications.

Features & Benefits

Superior Weather Resistance

Tairilac WE830M withstands harsh UV exposure and extreme temperatures without fading or cracking, ensuring long-term performance in outdoor environments like roofing systems.

High Mechanical Strength

With a tensile strength of 29 MPa and flexural modulus of 1,400 MPa, this FCFC ASA Resin delivers structural integrity for load-bearing applications, reducing material failure risks.

Easy Processing&Consistency

Pre-drying at 80–85°C (2–3 hours) and compatibility with extrusion/injection molding streamline production, minimizing downtime and ensuring uniform product quality.

fcfc tairilac asa resin particles

Use & applications

Plastic Roof Tiles

Modified for enhanced UV resistance and durability in roofing systems.

Outdoor Construction Profiles

Ideal for fascia, cladding, and trim exposed to weathering.

Automotive Exteriors

Suitable for non-structural parts requiring color retention and impact resistance.

tairilac asa resin we830m application

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.