FCFC Formosa TAIRILAC® WE9100 ASA

fcfc tairilac® asa resin 25kg package

TAIRILAC® WE9100 Weathering Grade ASA Resin

FCFC TAIRILAC WE9100 ASA Resin is a high-performance, weather-resistant polymer designed for demanding outdoor applications. Ideal for plastic roof tile modification, this milky off-white pellet combines exceptional UV stability, mechanical strength, and thermal resistance, ensuring long-term durability in harsh environments.

Associated Documents

ISO Data Sheet
ASTM Data Sheet

Typical property data

Physical Properties
  • Melt Flow Index: 1.8 g/10 min (ISO 1133, 220°C × 10 kg)
  • Specific Gravity: 1.05 (ISO 1183, 23°C/23°C)
Mechanical Properties
  • Tensile Strength: 18 MPa (ISO 527, 23°C, 50 mm/min)
  • Flexural Strength: 22 MPa (ISO 178, 23°C, 2 mm/min)
  • Flexural Modulus: 1000 MPa (ISO 178, 23°C, 2 mm/min)
  • Charpy Impact Strength: 65 kJ/m² (ISO 179, 23°C, 4 mm thickness, Notched)
  • Rockwell Hardness: R-53 (ISO 2039-2, 23°C)
Thermal Properties
  • Vicat Softening Point: 83°C (ISO 306, Annealed, 50 N, 50°C/h)
  • Heat Deflection Temperature: 84°C (ISO 75/A, Annealed, 1.8 MPa, 4 mm thickness, 120°C/h)
Other Properties

Molding Shrinkage: 0.4–0.7% (ISO 2577, 3.2 mm thickness)

Features & Benefits

Superior Weather Resistance

TAIRILAC WE9100 excels in UV stability, preventing color fading and brittleness even under prolonged sun exposure. Perfect for outdoor products like roofing, signage, and cladding.

High Impact Strength

With a Charpy Impact Strength of 65 kJ/m² (ISO 179), this ASA resin withstands mechanical stress, reducing breakage risks in auto parts, junction boxes, and industrial components.

Reliable Thermal Stability

Boasting a Heat Deflection Temperature of 84°C (ISO 75/A), TAIRILAC ASA WE9100 maintains structural integrity in high-temperature environments, ideal for automotive under-hood parts.

fcfc tairilac asa resin particles

Use & applications

Outdoor Products

Durable roofing tiles, garden equipment, and architectural panels resistant to UV and moisture.

Junction Boxes

Robust enclosures for electrical systems, ensuring safety in extreme weather conditions.

Auto Parts

Exterior trims, mirror housings, and under-hood components withstanding heat and impact.