FCFC Formosa TAIRIPRO® F4006 PP Random Copolymer

fcfc tairipro pp resin random copolymer

TAIRIPRO® F4006 Random Copolymer PP Film Grade

TAIRIPRO® F4006 is a premium random copolymer polypropylene resin designed for exceptional transparency and versatility. It delivers balanced processability and lightweight performance. Its high clarity makes it ideal for applications requiring visual appeal, such as food packaging and consumer goods. Certified under ISO standards, F4006 combines durability with aesthetic flexibility for injection molding and film production.

Associated Documents

ISO Data Sheet
ASTM Data Sheet
Processing Data

Typical property data

Physical Properties
  • Melt Flow Index: 7.5 g/10 min (ISO 1133, 230°C × 2.16 kg)
  • Specific Gravity: 0.9 (ISO 1183, 23°C)
Mechanical Properties
  • Tensile Strength: 25 MPa (ISO 527, 23°C, 50 mm/min)
  • Tensile Elongation at Break: >200% (ISO 527, 23°C, 50 mm/min)
  • Flexural Modulus: 833 MPa (ISO 178, 23°C)
  • Rockwell Hardness: R-85 (R-scale, ISO 2039-2, 23°C)
Impact Properties
  • IZOD Impact Strength: 64 kJ/m² (ISO 180, 23°C, Notched, 1/8 inch and 4 mm)
Thermal Properties
  • Heat Deflection Temperature (HDT): 85°C (ISO 75/A, Unannealed, 0.455 MPa, 1/4 inch, 120°C/h)
Optical Properties
  • Good transparency (general observation)
Injection Molding
  • Molding Shrinkage: 1.5–2% (FCFC Method, 23°C)

Features & Benefits

Crystal-Clear Aesthetics

Superior transparency enhances visual appeal, perfect for see-through packaging, medical devices, and premium consumer products where clarity matters.

Reliable Impact Resistance

With an IZOD impact strength of 64 kJ/m², this Tairipro PP resin resists cracks and drops, ensuring longevity in automotive parts, storage containers, and heavy-duty packaging.

Heat-Resistant Performance

Stable up to 85°C, it maintains integrity during sterilization or hot-fill processes, making it suitable for medical tools and heat-exposed industrial applications.

fcfc tairipro pp resin random copolymer

Use & applications

Industrial Films

Transparent lids, microwave-safe trays.

Industrial Films

BOPP films for labels, adhesive tapes.

Medical Devices

Sterile packaging with chemical resistance.

tairipro f4006 pp resin application

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.