Plastic Granules
TAIRIPRO® F4007 Random Copolymer PP Film Grade
TAIRIPRO F4007 is a high-performance random copolymer polypropylene resin designed to deliver exceptional transparency and balanced mechanical properties. This versatile Tairipro PP resin offers excellent processability with a melt flow index of 7.5 g/10 min, making it ideal for applications requiring clarity, impact resistance, and reliable performance across various processing conditions.
Associated Documents
ISO Data Sheet
ASTM Data Sheet
MSDS
Processing Data
Typical property data
Physical Properties
- Melt Flow Index: 7.5 g/10 min (ISO 1133, 230°C × 2.16 kg)
- Specific Gravity: 0.9 (ISO 1183, 23°C/23°C)
Mechanical Properties
- Tensile Strength: 25 MPa (ISO 527, 23°C, 50 mm/min)
- Tensile Elongation at Break: >200% (ISO 527, 23°C, 50 mm/min)
- Flexural Modulus: 833 MPa (ISO 178, 23°C)
- Rockwell Hardness: R-85 (R-scale, ISO 2039-2, 23°C)
Impact Properties
IZOD Impact Strength: 64 kJ/m² (ISO 180, 23°C, Notched, 1/8″ and 4 mm)
Thermal Properties
Heat Deflection Temperature (HDT): 85°C (ISO 75/A, Unannealed, 0.455 MPa, 1/4″ thick, 120°C/h)
Optical Properties
Features: Good transparency
Injection Molding
Molding Shrinkage: 1.5–2% (FCFC Method, 23°C)
Features & Benefits
Crystal-Clear Visibility Performance
F4007’s high transparency rivals traditional plastics like PET, making it perfect for packaging, medical devices, and containers where visual appeal matters. Its light-diffusing properties reduce the need for additives, lowering production costs.
Chemical & Heat Resilience
It resists acids, alcohols, and steam sterilization (heat deflection temperature: 85°C), ensuring durability in chemical storage containers, healthcare tools, and sterilizable packaging without compromising structural integrity.
Impact-Resistant Formula
With an IZOD impact strength of 64 kJ/m², this resin, this resin withstands drops, impacts, and harsh handling—ideal for blow-molded bottles, automotive components, and industrial parts prone to mechanical stress.
Use & applications
Blow Molding
Lightweight bottles, containers, and automotive ducts with high clarity and crack resistance.
USP CLASS VI Approved
Safe for medical devices, IV components, and pharmaceutical packaging.
Transparent Films
Food-grade packaging, shrink wraps, and display covers requiring scratch-resistant clarity.
Household Goods
Durable housewares, storage bins, and toys with a glossy finish.